Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 8.25 MPa @Strain 7.41 %, Temperature 150 °C |
1200 psi @Strain 7.41 %, Temperature 302 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Crastin® 6129 NC010 Polybutylene Terephthalate (PBT)
(Unverified Data**) Unreinforced High Viscosity Polybutylene Terephthalate Developed for Extrusion and Injection MoldingInformation provided by DuPont Performance Polymers |
|||
Tensile Stress | 8.25 MPa @Strain 7.41 %, Temperature 150 °C |
1200 psi @Strain 7.41 %, Temperature 302 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Crastin® 6130 NC010 Polybutylene Terephthalate (PBT)
(Unverified Data**) Unreinforced High Viscosity Polybutylene Terephthalate Developed for Extrusion and Injection Molding Crastin 6130 NC010 is an unreinforced medium high viscosity polybutylene terephthalate resin for .. |