Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 8.13 MPa @Strain 87.33 %, Temperature 120 °C |
1180 psi @Strain 87.33 %, Temperature 248 °F |
TPE; ISO 11403-1 -2 |
DuPont Performance Polymers Hytrel® 6359FG NC010 Polyester Elastomer TPC-ET
(Unverified Data**) 63 Shore D High Performance Polyester Elastomer Developed for Food Contact ApplicationsInformation provided by DuPont Performance Polymers |
|||
Tensile Stress | 8.13 MPa @Strain 0.110 %, Temperature 40.0 °C |
1180 psi @Strain 0.110 %, Temperature 104 °F |
50%RH; ISO 11403-1/-2 |
DuPont Performance Polymers Zytel® PLUS PLS93G35DH1 BK261 Nylon 6
(Unverified Data**) Zytel® PLS93G35DH1 BK261 is a 35% glass reinforced PA6 using SHIELD Technology, only from DuPont, it provides exceptional welding resistance & retention over time thanks to excellent Heat Resistanc.. |
|||
Tensile Stress | 8.13 MPa @Strain 0.0400 %, Temperature 23.0 °C |
1180 psi @Strain 0.0400 %, Temperature 73.4 °F |
50%RH; ISO 11403-1/-2 |
DuPont Performance Polymers Zytel® PLUS PLS95G50DH2 BK261 Nylon
(Unverified Data**) Zytel® PLS95G50DH2 BK261is a high flow 50% glass reinforced PA nylon resin using SHIELD Technology, only from DuPont providing exceptional Heat Resistance & High stiffness for automotive under hood.. |