Tensile Stress 54.78 MPa

@Strain 2.40 %,
Temperature 0.000 °C
7945 psi

@Strain 2.40 %,
Temperature 32.0 °F
ISO 11403-1 -2
DuPont Performance Polymers Crastin® 6129 NC010 Polybutylene Terephthalate (PBT)  (Unverified Data**)
Unreinforced High Viscosity Polybutylene Terephthalate Developed for Extrusion and Injection MoldingInformation provided by DuPont Performance Polymers
Tensile Stress 54.78 MPa

@Strain 2.40 %,
Temperature 0.000 °C
7945 psi

@Strain 2.40 %,
Temperature 32.0 °F
ISO 11403-1 -2
DuPont Performance Polymers Crastin® 6130 NC010 Polybutylene Terephthalate (PBT)  (Unverified Data**)
Unreinforced High Viscosity Polybutylene Terephthalate Developed for Extrusion and Injection Molding Crastin 6130 NC010 is an unreinforced medium high viscosity polybutylene terephthalate resin for ..