Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 5.17 MPa @Strain 300 % |
750 psi @Strain 300 % |
510 mm/min; ASTM D412A |
PolyOne Elastamax™ EG-9177 Thermoplastic Elastomer (TPE) The Elastamax™ EG 9100 Series is a new family of olefin-based TPE compounds offering outstanding elastomeric performance in a lightweight and easy to process material. The EG 9100 Series of compoun.. |
|||
Tensile Stress | 5.17 MPa @Strain 300 % |
750 psi @Strain 300 % |
ASTM D412 |
Teknor Apex Telcar® TL-1025-75 Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets P.. |
|||
Tensile Stress | 5.17 MPa @Strain 0.0600 %, Temperature 150 °C |
750 psi @Strain 0.0600 %, Temperature 302 °F |
DAM; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® HTN 53G60LRHF BK083 Polyphthalamide (PPA)
(Unverified Data**) 60% Glass Reinforced High Performance Polyamide with High Stiffness and Improved Flow Zytel HTN53G60LRHF BK083 is a 60% glass reinforced lubricated high performance polyamide resin with improved flo.. |
|||
Tensile Stress | 5.17 MPa @Strain 0.0500 %, Temperature 120 °C |
750 psi @Strain 0.0500 %, Temperature 248 °F |
50%RH; ISO 11403-1/-2 |
DuPont Performance Polymers Zytel® PLUS PLS95G50DH2 BK261 Nylon
(Unverified Data**) Zytel® PLS95G50DH2 BK261is a high flow 50% glass reinforced PA nylon resin using SHIELD Technology, only from DuPont providing exceptional Heat Resistance & High stiffness for automotive under hood.. |