Mechanical Properties Metric English Comments
Tensile Stress 51.39 MPa

@Strain 2.00 %,
Temperature -20.0 °C
7454 psi

@Strain 2.00 %,
Temperature -4.00 °F
ISO 11403-1 -2
DuPont Performance Polymers Crastin® 6129 NC010 Polybutylene Terephthalate (PBT)  (Unverified Data**)
Unreinforced High Viscosity Polybutylene Terephthalate Developed for Extrusion and Injection MoldingInformation provided by DuPont Performance Polymers
Tensile Stress 51.39 MPa

@Strain 2.00 %,
Temperature -20.0 °C
7454 psi

@Strain 2.00 %,
Temperature -4.00 °F
ISO 11403-1 -2
DuPont Performance Polymers Crastin® 6130 NC010 Polybutylene Terephthalate (PBT)  (Unverified Data**)
Unreinforced High Viscosity Polybutylene Terephthalate Developed for Extrusion and Injection Molding Crastin 6130 NC010 is an unreinforced medium high viscosity polybutylene terephthalate resin for ..
Tensile Stress 51.39 MPa

@Strain 2.50 %,
Temperature 150 °C
7454 psi

@Strain 2.50 %,
Temperature 302 °F
DAM; ISO 11403-1/-2
DuPont Performance Polymers Zytel® PLUS PLS95G40DH1T BK261 Nylon  (Unverified Data**)
Zytel® PLS95G40DH1T is a 40% GR impact modified PA, made with SHIELD technology, its superior heat & oil resistance combined with the "stone impact resistance" makes it ideal choice for use in seve..