Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 5.10 MPa @Strain 300 % |
740 psi @Strain 300 % |
ISO 37 |
PolyOne OnFlex™ S HF 90A-3S1988 Thermoplastic Elastomer (TPE) OnFlex™-S HF thermoplastic elastomer compounds are based on hydrogenated styrenic block copolymers. This range of compounds utilize a unique, patent pending halogen free flame retardancy system. Fu.. |
|||
Tensile Stress | 5.10 MPa @Strain 100 % |
740 psi @Strain 100 % |
ASTM D412 |
Teknor Apex Monprene® MP-1848K Thermoplastic Elastomer Uses: Wire and Cable ApplicationsForms: Pellets Processing Method: Extrusion; Injection Molding Injection Notes: Drying is not necessary. However, if moisture is a problem, dry the pellets for 2 to.. |
|||
Tensile Stress | 5.10 MPa @Strain 25.0 % |
740 psi @Strain 25.0 % |
Average; ASTM D412 Method A |
Seals Eastern 7042 Fluorocarbon-Elastomer Seals Eastern's formulated Viton® elastomers can be utilized in seals, o-rings, gaskets, packings and other applications where thermal stability and chemical resistance are required.Features:Type.. |
|||
Tensile Stress | 5.10 MPa @Strain 5.00 % |
740 psi @Strain 5.00 % |
ISO 527-1/-2 |
DSM Arnitel® VT3108 TPC-ET Extrusion Grade, High Breathable, Drying of Material Required |
|||
Tensile Stress | 5.10 MPa @Strain 100 % |
740 psi @Strain 100 % |
ISO 527-1/-2 |
DSM Arnitel® EL250 TPC-ET Injection Molding |
|||
Tensile Stress | 5.10 MPa @Strain 6.00 %, Temperature 23.0 °C |
740 psi @Strain 6.00 %, Temperature 73.4 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Hytrel® G4774 Polyester Elastomer TPC-ET
(Unverified Data**) 47 Shore D Standard Performance Polyester Elastomer with Heat Ageing ProtectionHytrel G4774 is a medium modulus grade with nominal hardness of 47D. It contains discoloring stabilizer. It can be proc.. |
|||
Tensile Stress | 5.10 MPa @Strain 5.00 %, Temperature 23.0 °C |
740 psi @Strain 5.00 %, Temperature 73.4 °F |
ISO 527 (1BA bar) |
DuPont Performance Polymers Hytrel® HTR5612BK TPC-ET
(Unverified Data**) Hytrel® HTR5612BK HTR5612BK is designed for blow molding or processing techniques requiring high melt viscosity. It has nominal durometer hardness of 54D, is pigmented black with fine particle size.. |
|||
Tensile Stress | 5.10 MPa @Strain 38.95 %, Temperature 120 °C |
740 psi @Strain 38.95 %, Temperature 248 °F |
TPE; ISO 11403-1 -2 |
DuPont Performance Polymers Hytrel® HTR8223 BK320 Polyester Elastomer TPC-ET
(Unverified Data**) 42 Shore D High Viscosity Polyester Elastomer Developed for Blow MoldingInformation provided by DuPont Performance Polymers |
|||
Tensile Stress | 5.10 MPa @Strain 100 % |
740 psi @Strain 100 % |
ISO 37 |
Alliance Polymers Viprene™ P85A-22U-NAT Thermoplastic Vulcanizate Elastomer Viprene™ P85A-22U-NAT is a UV and Heat Stabilized TVP (Thermoplastic Vulcanizate Elastomer). This material can be easily processed by extrusion or injection molding. It exhibits easy flowing charac.. |
|||
Tensile Stress | 5.10 MPa @Strain 100 % |
740 psi @Strain 100 % |
ISO 37 |
Alliance Polymers Viprene™ P85A-22U-BLK Thermoplastic Vulcanizate Elastomer Viprene™ P85A-22U-BLK is a UV and Heat Stabilized TVP (Thermoplastic Vulcanizate Elastomer). This material can be easily processed by extrusion or injection molding. It exhibits easy flowing charac.. |