Material Notes:
Extrusion Grade, High Breathable, Drying of Material Required
Physical Properties Metric English Comments
Density 1.25 g/cc
0.0452 lb/in³
ISO 1183
Water Absorption 33 %
33 %
Sim. To ISO 62
Melt Flow 10 g/10 min

@Load 2.16 kg,
Temperature 230 °C
10 g/10 min

@Load 4.76 lb,
Temperature 446 °F
cm<sup>3</sup>/10min Melt Volume-flow Rate; ISO 1133
Mechanical Properties Metric English Comments
Hardness, Shore D 45

@Time 3.00 sec
45

@Time 0.000833 hour
ISO 868
Tensile Strength, Ultimate 20.0 MPa
2900 psi
ISO 527-1/-2
Tensile Stress 5.10 MPa

@Strain 5.00 %
740 psi

@Strain 5.00 %
ISO 527-1/-2
8.10 MPa

@Strain 10.0 %
1170 psi

@Strain 10.0 %
ISO 527-1/-2
12.5 MPa

@Strain 50.0 %
1810 psi

@Strain 50.0 %
ISO 527-1/-2
14.1 MPa

@Strain 100 %
2050 psi

@Strain 100 %
ISO 527-1/-2
Elongation at Break 280 %
280 %
ISO 527-1/-2
Tensile Modulus 0.110 GPa
16.0 ksi
ISO 527-1/-2
Izod Impact Resistance NB

@Temperature 23.0 °C
NB

@Temperature 73.4 °F
ISO 180/1A
NB

@Temperature -30.0 °C
NB

@Temperature -22.0 °F
ISO 180/1A
Charpy Impact, Notched NB

@Temperature 23.0 °C
NB

@Temperature 73.4 °F
ISO 179/1eA
NB

@Temperature -30.0 °C
NB

@Temperature -22.0 °F
ISO 179/1eA
Thermal Properties Metric English Comments
Melting Point 185 °C
365 °F
10°C/min; ISO 11357-1/-3