Polymer Property : Tensile Stress = 7.60 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Stress 7.60 MPa

@Strain 100 %
1100 psi

@Strain 100 %
ISO 37
PolyOne OnFlex™ V 3040D-S0093 Thermoplastic Elastomer (TPE)
OnFlex™-V provides the performance of traditional vulcanised rubber, but with the processability of a thermoplastic. OnFlex™-V 3000 series thermoplastic elastomer compounds are based on a polyolef..
Tensile Stress 7.60 MPa

@Strain 0.100 %,
Temperature 0.000 °C
1100 psi

@Strain 0.100 %,
Temperature 32.0 °F
DAM; ISO 11403-1 -2
DuPont Performance Polymers Minlon® 22C NC010 Nylon 66  (Unverified Data**)
38% Mineral/Glass Reinforced Polyamide 66 Minlon 22C NC010 is a 38% mineral/glass reinforced heat stabilized polyamide 66 resin for injection molding.Information provided by DuPont Performance Polym..
Tensile Stress 7.60 MPa

@Strain 0.250 %,
Temperature 23.0 °C
1100 psi

@Strain 0.250 %,
Temperature 73.4 °F
50%RH; ISO 11403-1 -2
DuPont Performance Polymers Zytel® 73G15L NC010 Nylon 6  (Unverified Data**)
15% Glass Reinforced Polyamide 6Zytel 73G15L NC010 is a 15% glass fiber reinforced polyamide 6 resin for injection molding.Information provided by DuPont Performance Polymers
Tensile Stress 7.60 MPa

@Strain 10.0 %
1100 psi

@Strain 10.0 %
ISO 527-1/-2
DuPont Performance Polymers Hytrel® HTR237BG BK320 Polyester Elastomer TPC-ET  (Unverified Data**)
45 Shore D Lubricated High Viscosity Polyester Elastomer Developed for Blow Molding Hytrel HTR237BG is designed for blow molding or processing techniques requiring high viscosity. It has nominal dur..
Tensile Stress 7.60 MPa

@Strain 5.00 %,
Temperature 23.0 °C
1100 psi

@Strain 5.00 %,
Temperature 73.4 °F
ASTM D638
DuPont Performance Polymers Hytrel® HTR6108 TPC-ET  (Unverified Data**)
Hytrel® HTR6108 is a medium modulus grade, specially designed for good flexibility and low permeability to hydrocarbon fuels and oils. It has nominal hardness of 61D and can be processed by various..