Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 46.1 MPa @Strain 0.360 %, Temperature 0.000 °C |
6690 psi @Strain 0.360 %, Temperature 32.0 °F |
50%RH; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® 70G43L NC010 Nylon 66
(Unverified Data**) 43% Glass Reinforced Polyamide 66Zytel 70G43L NC010 is a 43% glass fiber reinforced polyamide 66 resin for injection molding.Information provided by DuPont Performance Polymers |
|||
Tensile Stress | 46.1 MPa @Strain 1.62 %, Temperature 90.0 °C |
6690 psi @Strain 1.62 %, Temperature 194 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Crastin® LW9020FR NC010 PBT+ASA
(Unverified Data**) 20% Glass Reinforced Flame Retardant Polybutylene Terephthalate Blend with Low Warpage Characteristics Crastin LW9020FR NC010 is a 20% glass fiber reinforced flame retardant polybutylene terephthal.. |