Mechanical Properties Metric English Comments
Tensile Stress 46.1 MPa

@Strain 0.360 %,
Temperature 0.000 °C
6690 psi

@Strain 0.360 %,
Temperature 32.0 °F
50%RH; ISO 11403-1 -2
DuPont Performance Polymers Zytel® 70G43L NC010 Nylon 66  (Unverified Data**)
43% Glass Reinforced Polyamide 66Zytel 70G43L NC010 is a 43% glass fiber reinforced polyamide 66 resin for injection molding.Information provided by DuPont Performance Polymers
Tensile Stress 46.1 MPa

@Strain 1.62 %,
Temperature 90.0 °C
6690 psi

@Strain 1.62 %,
Temperature 194 °F
ISO 11403-1 -2
DuPont Performance Polymers Crastin® LW9020FR NC010 PBT+ASA  (Unverified Data**)
20% Glass Reinforced Flame Retardant Polybutylene Terephthalate Blend with Low Warpage Characteristics Crastin LW9020FR NC010 is a 20% glass fiber reinforced flame retardant polybutylene terephthal..