Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 44.2 MPa @Strain 5.50 %, Temperature 40.0 °C |
6410 psi @Strain 5.50 %, Temperature 104 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Delrin® 500T NC010 Acetal (POM)
(Unverified Data**) Toughened Medium Viscosity Acetal Homopolymer Delrin 500T NC010 is a toughened medium viscosity acetal homopolymer resin with impact resistance similar to Delrin 100. It can be used in parts requiri.. |
|||
Tensile Stress | 44.2 MPa @Strain 0.900 %, Temperature 23.0 °C |
6410 psi @Strain 0.900 %, Temperature 73.4 °F |
DAM; ISO 11403-1 -2 |
DuPont Performance Polymers Minlon® 12T NC010 Nylon 66
(Unverified Data**) 36% Mineral Reinforced Toughened Polyamide 66 Minlon 12T NC010 is a 36% mineral reinforced toughened heat stabilized polyamide 66 resin for injection molding.Information provided by DuPont Performan.. |