Mechanical Properties Metric English Comments
Tensile Stress 44.2 MPa

@Strain 5.50 %,
Temperature 40.0 °C
6410 psi

@Strain 5.50 %,
Temperature 104 °F
ISO 11403-1 -2
DuPont Performance Polymers Delrin® 500T NC010 Acetal (POM)  (Unverified Data**)
Toughened Medium Viscosity Acetal Homopolymer Delrin 500T NC010 is a toughened medium viscosity acetal homopolymer resin with impact resistance similar to Delrin 100. It can be used in parts requiri..
Tensile Stress 44.2 MPa

@Strain 0.900 %,
Temperature 23.0 °C
6410 psi

@Strain 0.900 %,
Temperature 73.4 °F
DAM; ISO 11403-1 -2
DuPont Performance Polymers Minlon® 12T NC010 Nylon 66  (Unverified Data**)
36% Mineral Reinforced Toughened Polyamide 66 Minlon 12T NC010 is a 36% mineral reinforced toughened heat stabilized polyamide 66 resin for injection molding.Information provided by DuPont Performan..