Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 6.36 MPa @Strain 80.48 %, Temperature 90.0 °C |
922 psi @Strain 80.48 %, Temperature 194 °F |
TPE; ISO 11403-1 -2 |
DuPont Performance Polymers Hytrel® 4556 Polyester Elastomer TPC-ET
(Unverified Data**) 45 Shore D High Performance Polyester ElastomerInformation provided by DuPont Performance Polymers |
|||
Tensile Stress | 6.36 MPa @Strain 0.0400 %, Temperature 60.0 °C |
922 psi @Strain 0.0400 %, Temperature 140 °F |
50%RH; ISO 11403-1/-2 |
DuPont Performance Polymers Zytel® PLUS PLS95G50DH2 BK261 Nylon
(Unverified Data**) Zytel® PLS95G50DH2 BK261is a high flow 50% glass reinforced PA nylon resin using SHIELD Technology, only from DuPont providing exceptional Heat Resistance & High stiffness for automotive under hood.. |