Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 4.08 MPa @Strain 6.86 %, Temperature -20.0 °C |
592 psi @Strain 6.86 %, Temperature -4.00 °F |
TPE; ISO 11403-1 -2 |
DuPont Performance Polymers Hytrel® 4068FG Polyester Elastomer TPC-ET
(Unverified Data**) 40 Shore D High Performance Polyester Elastomer Developed for Food Contact ApplicationsInformation provided by DuPont Performance Polymers |
|||
Tensile Stress | 4.08 MPa @Strain 0.0600 %, Temperature 150 °C |
592 psi @Strain 0.0600 %, Temperature 302 °F |
50%RH; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® HTN 53G60LRHF BK083 Polyphthalamide (PPA)
(Unverified Data**) 60% Glass Reinforced High Performance Polyamide with High Stiffness and Improved Flow Zytel HTN53G60LRHF BK083 is a 60% glass reinforced lubricated high performance polyamide resin with improved flo.. |