Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 3.86 MPa @Strain 300 % |
560 psi @Strain 300 % |
|
NEU NeuSoft™ 602-50A Ester TPU / SBC blend |
|||
Tensile Stress | 3.86 MPa @Strain 100 % |
560 psi @Strain 100 % |
ASTM D412 |
Teknor Apex Monprene® MP-1848R Thermoplastic Elastomer Uses: Wire and Cable ApplicationsForms: Pellets Processing Method: Extrusion; Injection Molding Injection Notes: Drying is not necessary. However, if moisture is a problem, dry the pellets for 2 to.. |
|||
Tensile Stress | 3.86 MPa @Strain 100 % |
560 psi @Strain 100 % |
ASTM D412 |
Teknor Apex Telcar® TL-1025-75 Thermoplastic Elastomer Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets P.. |
|||
Tensile Stress | 3.86 MPa @Strain 52.82 %, Temperature 90.0 °C |
560 psi @Strain 52.82 %, Temperature 194 °F |
TPE; ISO 11403-1 -2 |
DuPont Performance Polymers Hytrel® 4056 Polyester Elastomer TPC-ET
(Unverified Data**) 40 Shore D High Performance Polyester ElastomerInformation provided by DuPont Performance Polymers |
|||
Tensile Stress | 3.86 MPa @Strain 73.94 %, Temperature 100 °C |
560 psi @Strain 73.94 %, Temperature 212 °F |
TPE; ISO 11403-1 -2 |
DuPont Performance Polymers Hytrel® 4068FG Polyester Elastomer TPC-ET
(Unverified Data**) 40 Shore D High Performance Polyester Elastomer Developed for Food Contact ApplicationsInformation provided by DuPont Performance Polymers |
|||
Tensile Stress | 3.86 MPa @Strain 0.0500 %, Temperature 150 °C |
560 psi @Strain 0.0500 %, Temperature 302 °F |
DAM; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® HTN 92G35DH2 BK083 Polyphthalamide (PPA)
(Unverified Data**) 35% Glass Reinforced PPA High Performance Polyamide with DuPont Zytel HTN92G35DH2 BK083 is a 35% glass reinforced high performance polyamide resin using DuPont SHIELD Technology with high flow and e.. |