Polymer Property : Tensile Stress = 56.48 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Stress 56.48 MPa

@Strain 2.29 %,
Temperature 0.000 °C
8192 psi

@Strain 2.29 %,
Temperature 32.0 °F
ISO 11403-1 -2
DuPont Performance Polymers Delrin® 311DP NC010 Acetal (POM)  (Unverified Data**)
Nucleated Medium-high Viscosity Acetal Homopolymer Delrin 311DP is a medium-high viscosity acetal homopolymer with enhanced crystallization and balance of part performance and ease of processing. It..
Tensile Stress 56.48 MPa

@Strain 2.29 %,
Temperature 0.000 °C
8192 psi

@Strain 2.29 %,
Temperature 32.0 °F
ISO 11403-1 -2
DuPont Performance Polymers Delrin® FG311DP NC010 Acetal (POM)  (Unverified Data**)
Nucleated Medium-high Viscosity Acetal Homopolymer Developed for Food Contact Applications Delrin FG311DP is a medium-high viscosity acetal homopolymer with improved thermal stability and modificati..
Tensile Stress 56.48 MPa

@Strain 0.200 %,
Temperature -20.0 °C
8192 psi

@Strain 0.200 %,
Temperature -4.00 °F
DAM; ISO 11403-1 -2
DuPont Performance Polymers Zytel® HTN 53G60LRHF BK083 Polyphthalamide (PPA)  (Unverified Data**)
60% Glass Reinforced High Performance Polyamide with High Stiffness and Improved Flow Zytel HTN53G60LRHF BK083 is a 60% glass reinforced lubricated high performance polyamide resin with improved flo..