Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 34.3 MPa @Strain 1.10 %, Temperature 0.000 °C |
4970 psi @Strain 1.10 %, Temperature 32.0 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Delrin® 500TL NC010 Acetal (POM)
(Unverified Data**) Teflon® Lubricated Medium Viscosity Acetal Homopolymer with Low Wear and Low Friction Delrin 500TL is a medium viscosity acetal homopolymer resin containing 1.5% Teflon PTFE Micropowder. It is desi.. |
|||
Tensile Stress | 34.3 MPa @Strain 1.10 %, Temperature 0.000 °C |
4970 psi @Strain 1.10 %, Temperature 32.0 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Delrin® FG500TL NC010 Acetal (POM)
(Unverified Data**) Teflon® Lubricated Medium Viscosity Acetal Homopolymer with Low Wear and Low Friction Developed for Food Contact ApplicationsDelrin FG500TL medium viscosity acetal homopolymer resin containing 1.5%.. |
|||
Tensile Stress | 34.3 MPa @Strain 2.60 %, Temperature 150 °C |
4970 psi @Strain 2.60 %, Temperature 302 °F |
50%RH; ISO 11403-1 -2 |
DuPont Performance Polymers Minlon® 22C NC010 Nylon 66
(Unverified Data**) 38% Mineral/Glass Reinforced Polyamide 66 Minlon 22C NC010 is a 38% mineral/glass reinforced heat stabilized polyamide 66 resin for injection molding.Information provided by DuPont Performance Polym.. |
|||
Tensile Stress | 34.3 MPa @Strain 300 %, Temperature -40.0 °C |
4970 psi @Strain 300 %, Temperature -40.0 °F |
ISO 527 (1BA bar) |
DuPont Performance Polymers Hytrel® HTR8636 NC010 TPC-ET
(Unverified Data**) Hytrel® HTR8636 NC010 is a medium modulus Hytrel® grade with nominal durometer hardness of 40D. It contains non_discoloring stabilizer. It is specially suitable for extrusion processing.Informatio.. |