Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 31.0 MPa @Strain 3.80 %, Temperature 40.0 °C |
4500 psi @Strain 3.80 %, Temperature 104 °F |
ISO 527 |
DuPont Performance Polymers Delrin® 100T NC010 Acetal Homopolymer
(Unverified Data**) Delrin® 100T NC010 is a toughened, high viscosity acetal homopolymer grade with high impact resistance.Information provided by DuPont Performance Polymers |
|||
Tensile Stress | 31.0 MPa @Strain 0.180 %, Temperature 23.0 °C |
4500 psi @Strain 0.180 %, Temperature 73.4 °F |
ISO 527 |
DuPont Performance Polymers Rynite® FR543 NC010 PET Rynite® FR543 NC010 is a flame retardant, 43% glass reinforced polyethylene terephthalate. Has a 155C temperature index that is equivalent to many thermosets. Recognized by UL as UL94V-0 at 0.8mm.. |
|||
Tensile Stress | 31.0 MPa @Strain 4.58 %, Temperature 180 °C |
4500 psi @Strain 4.58 %, Temperature 356 °F |
50%RH; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® BM70G20HSLX BK537 Nylon 66
(Unverified Data**) 20% Glass Reinforced Heat Stabilized Polyamide 66 Developed for Blow Molding Zytel BM70G20HSLX BK537 is a 20% glass fiber reinforced polyamide 66 for blow molding.Information provided by DuPont Perf.. |
|||
Tensile Stress | 31.0 MPa @Strain 300 % |
4500 psi @Strain 300 % |
ASTM D412 |
Alliance Polymers Zythane™ 3045D Thermoplastic Polyurethane Elastomer Zythane™ 3045D is a polycaprolactone-based TPU specifically formulated for injection molding applications .It exhibits excellent low compression set, abrasion resistance and toughness and has good .. |
|||
Tensile Stress | 31.0 MPa @Strain 0.600 %, Time 3.60e+6 sec |
4500 psi @Strain 0.600 %, Time 1000 hour |
ISO 899-1 |
BASF Ultraform N 2200 G53 UNC Q600 25% Glass Filled POM Ultraform N2200 G53 UNC Q600 is a 25% glass fiber reinforced POM injection molding grade with enhanced stiffness and toughness. |
|||
Tensile Stress | 31.0 MPa @Time 3600 sec, Strain 2.00 % |
4500 psi @Time 1.00 hour, Strain 2.00 % |
ISO 899-1 |
BASF Ultraform N 2320 003 UNC Q600 POM Ultraform N 2320 003 UNC Q600 is a rapidly solidifying grade of POM for injection molding. Contains a mold release agent. |
|||
Tensile Stress | 31.0 MPa @# of Cycles 1.00e+7 , Temperature 180 °C |
4500 psi @# of Cycles 1.00e+7 , Temperature 356 °F |
|
BASF Ultrason E 2010 G6 30% Glass Filled PES Ultrason E 2010 G6 is a 30% glass reinforced, medium viscosity injection molding PES grade with high rigidity and strength. |
|||
Tensile Stress | 31.0 MPa @Strain 50.0 %, Temperature 100 °C |
4500 psi @Strain 50.0 %, Temperature 212 °F |
50%RH; ISO 527 |
DuPont Performance Polymers Zytel® MT409AHS BK010 Nylon 66
(Unverified Data**) Zytel® MT409AHS BK010 is a Medium Toughened, high performance, heat stabilized, black polyamide 66 resin having good stiffness and improved knit line strength with superior toughness and processabi.. |
|||
Tensile Stress | 31.0 MPa @Strain 1.56 %, Temperature 60.0 °C |
4500 psi @Strain 1.56 %, Temperature 140 °F |
DAM; ISO 11403-1/-2 |
DuPont Performance Polymers Crastin® HR5315HF NC010 PBT
(Unverified Data**) Crastin® HR5315HF is a 15% glass reinforced PBT with high flow (HF), moderately toughened, hydrolysis resistant (HR) resin. Excellent balance of properties between terminal pullout and impact resis.. |