Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Tensile Stress = 44.9 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Stress 44.9 MPa

@Strain 2.20 %,
Temperature 23.0 °C
6510 psi

@Strain 2.20 %,
Temperature 73.4 °F
ISO 11403-1 -2
DuPont Performance Polymers Delrin® 100AL NC010 Acetal (POM)  (Unverified Data**)
Lubricated High Viscosity Acetal Homopolymer with Low Wear and Low Friction Delrin 100AL NC010 an unreinforced high viscosity lubricated acetal homopolymer resin containing an advanced system of lub..
Tensile Stress 44.9 MPa

@Strain 12.1 %,
Temperature 0.000 °C
6510 psi

@Strain 12.1 %,
Temperature 32.0 °F
ISO 11403-1 -2
DuPont Performance Polymers Delrin® 100ST NC010 Acetal (POM)  (Unverified Data**)
Super Toughened High Viscosity Acetal Homopolymer Delrin 100ST NC010 is a super tough high viscosity acetal homopolymer grade with superior impact resistance. It is designed for highly stressed part..
Tensile Stress 44.9 MPa

@Strain 2.20 %,
Temperature 23.0 °C
6510 psi

@Strain 2.20 %,
Temperature 73.4 °F
ISO 11403-1 -2
DuPont Performance Polymers Delrin® FG100AL NC010 Acetal (POM)  (Unverified Data**)
Lubricated High Viscosity Acetal Homopolymer with Low Wear and Low Friction Developed for Food Contact Applications Delrin FG100AL is a high viscosity lubricated acetal homopolymer resin containing ..
Tensile Stress 44.9 MPa

@Strain 6.28 %,
Temperature -20.0 °C
6510 psi

@Strain 6.28 %,
Temperature -4.00 °F
ISO 11403-1 -2
DuPont Performance Polymers Hytrel® 7246HS NC010 Polyester Elastomer TPC-ET  (Unverified Data**)
72 Shore D High Performance Polyester Elastomer with Heat Ageing Protection Hytrel 7246HS NC010 is a high modulus heat stabilized grade with nominal hardness of 72D.Information provided by DuPont Pe..
Tensile Stress 44.9 MPa

@Strain 0.460 %,
Temperature 0.000 °C
6510 psi

@Strain 0.460 %,
Temperature 32.0 °F
ISO 527
DuPont Performance Polymers Rynite® 408 NC010 PET
Rynite® 408 NC010 is a 30% glass reinforced modified polyethylene terephthalate with improved impact resistance. Excellent balance of strength, stiffness, toughness, and temperature resistance.Inf..
Tensile Stress 44.9 MPa

@Strain 21.2 %,
Temperature 40.0 °C
6510 psi

@Strain 21.2 %,
Temperature 104 °F
DAM; ISO 11403-1 -2
DuPont Performance Polymers Zytel® 158 NC010 Nylon 612  (Unverified Data**)
Unreinforced Polyamide 612Zytel 158 NC010 is an intermediate viscosity PA 612 resin.Information provided by DuPont Performance Polymers
Tensile Stress 44.9 MPa

@Strain 7.40 %,
Temperature 23.0 °C
6510 psi

@Strain 7.40 %,
Temperature 73.4 °F
50%RH; ISO 11403-1 -2
DuPont Performance Polymers Zytel® 158 NC010 Nylon 612  (Unverified Data**)
Unreinforced Polyamide 612Zytel 158 NC010 is an intermediate viscosity PA 612 resin.Information provided by DuPont Performance Polymers
Copyright © lookpolymers.com All Rights Reserved