Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 2.54 MPa @Strain 300 %, Temperature 23.0 °C |
368 psi @Strain 300 %, Temperature 73.4 °F |
Die C2 hr; ASTM D412 |
PolyOne Versaflex™ HC 2110-43N Thermoplastic Elastomer (TPE) Versaflex™ HC 2110-43N is a unique TPE designed for the demanding requirements of gaskets and stoppers used in healthcare and food packaging applications. New Product. Commercial specifications hav.. |
|||
Tensile Stress | 2.54 MPa @Strain 100 %, Temperature 23.0 °C |
368 psi @Strain 100 %, Temperature 73.4 °F |
Die C2 hr; ASTM D412 |
PolyOne Versaflex™ HC 2110-57B Thermoplastic Elastomer (TPE) Versaflex™ HC 2110-57B is a TPE designed for use in the healthcare industry offering low stiction and good compression set. New Product. Commercial specifications have not been established. - Bonds.. |
|||
Tensile Stress | 2.54 MPa @Strain 3.88 %, Temperature 100 °C |
368 psi @Strain 3.88 %, Temperature 212 °F |
TPE; ISO 11403-1 -2 |
DuPont Performance Polymers Hytrel® HTR4275 BK316 Polyester Elastomer TPC-ET
(Unverified Data**) 55 Shore D High Viscosity Polyester Elastomer with Good Heat Ageing Protection Developed for Blow Molding Hytrel HTR4275 BK316 is designed for blow molding or processing techniques requiring high me.. |
|||
Tensile Stress | 2.54 MPa @Strain 3.88 %, Temperature 100 °C |
368 psi @Strain 3.88 %, Temperature 212 °F |
TPE; ISO 11403-1 -2 |
DuPont Performance Polymers Hytrel® RS R4275 BK316 Polyester Elastomer TPC-ET 55 Shore D Renewably Sourced High Viscosity Polyester Elastomer with Good Heat Ageing Protection Developed for Blow Molding Information provided by DuPont Performance Polymers |