Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 36.0 MPa @Strain 2.64 %, Temperature 0.000 °C |
5220 psi @Strain 2.64 %, Temperature 32.0 °F |
ISO 527 |
DuPont Performance Polymers Delrin® 100T NC010 Acetal Homopolymer
(Unverified Data**) Delrin® 100T NC010 is a toughened, high viscosity acetal homopolymer grade with high impact resistance.Information provided by DuPont Performance Polymers |
|||
Tensile Stress | 36.0 MPa @Strain 2.60 %, Temperature 0.000 °C |
5220 psi @Strain 2.60 %, Temperature 32.0 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Delrin® 100T NC010 Acetal (POM)
(Unverified Data**) Toughened High Viscosity Acetal Homopolymer Delrin 100T NC010 is a toughened high viscosity acetal homopolymer grade with high impact resistance.Information provided by DuPont Performance Polymers |
|||
Tensile Stress | 36.0 MPa @Strain 12.5 %, Temperature 40.0 °C |
5220 psi @Strain 12.5 %, Temperature 104 °F |
50%RH; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® RS LC1000 BK385 Nylon 1010 UV Stabilized Renewably Sourced Polyamide 1010 Developed for Extrusion Zytel RS LC1000 BK385 is a renewable sourced Polyamide 1010 containing a minimum of 90% renewably sourced ingredient by weight... |
|||
Tensile Stress | 36.0 MPa @Strain 50.0 %, Temperature 60.0 °C |
5220 psi @Strain 50.0 %, Temperature 140 °F |
50%RH; ISO 527 |
DuPont Performance Polymers Zytel® MT409AHS BK010 Nylon 66
(Unverified Data**) Zytel® MT409AHS BK010 is a Medium Toughened, high performance, heat stabilized, black polyamide 66 resin having good stiffness and improved knit line strength with superior toughness and processabi.. |