Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 34.5 MPa @Strain 12.0 %, Temperature 60.0 °C |
5000 psi @Strain 12.0 %, Temperature 140 °F |
ISO 527 |
DuPont Performance Polymers Delrin® 100T NC010 Acetal Homopolymer
(Unverified Data**) Delrin® 100T NC010 is a toughened, high viscosity acetal homopolymer grade with high impact resistance.Information provided by DuPont Performance Polymers |
|||
Tensile Stress | 34.5 MPa @Strain 1.50 %, Temperature 150 °C |
5000 psi @Strain 1.50 %, Temperature 302 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Crastin® SK645FR NC010 Polybutylene Terephthalate (PBT)
(Unverified Data**)&l 30% Glass Reinforced Flame Retardant Polybutylene Terephthalate Crastin SK645FR is a flame retardant 30% glass reinforced polybutylene terephthalate molding resin. It is recognized as UL94V-0 at 0.7.. |
|||
Tensile Stress | 34.5 MPa @Strain 0.100 % |
5000 psi @Strain 0.100 % |
|
COI Ceramics Nextel™ AS-N312 Oxide Ceramic Matrix Composite, Aluminosilicate Description: Oxide ceramic matrix composites products are based upon sol-gel derived matrices and 3M Corporation's Nextel™ fiber products. These materials can be used up to 1200ºC (2200ºF) in air.. |