Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 2.20 MPa @Strain 300 % |
319 psi @Strain 300 % |
ISO 37 |
PolyOne OnFlex™ S EH 50A-3S7002 Thermoplastic Elastomer (TPE) OnFlex™ S EH thermoplastic elastomer compounds are based on hydrogenated styrenic block copolymers. This range of compounds are formulated to deliver a great cost/performance ratio in addition to t.. |
|||
Tensile Stress | 2.20 MPa @Strain 100 % |
319 psi @Strain 100 % |
ISO 37 |
PolyOne OnFlex™ S KE 60A-3S1725 Thermoplastic Elastomer (TPE) OnFlex™-S KE thermoplastic elastomer compounds are based on hydrogenated styrenic block copolymers. This range of compounds are specially compatabilized to provide excellent adhesion to a variety p.. |
|||
Tensile Stress | 2.20 MPa @Strain 300 % |
319 psi @Strain 300 % |
ISO 37 |
PolyOne OnFlex™ S KG 40A-3S2016 Thermoplastic Elastomer (TPE) OnFlex™-S KG thermoplastic elastomer compounds are based on hydrogenated styrenic block copolymers. This range of compounds are specially compatabilized to provide excellent adhesion to polyamide p.. |
|||
Tensile Stress | 2.20 MPa @Strain 16.44 %, Temperature 120 °C |
319 psi @Strain 16.44 %, Temperature 248 °F |
TPE; ISO 11403-1 -2 |
DuPont Performance Polymers Hytrel® 4068FG Polyester Elastomer TPC-ET
(Unverified Data**) 40 Shore D High Performance Polyester Elastomer Developed for Food Contact ApplicationsInformation provided by DuPont Performance Polymers |
|||
Tensile Stress | 2.20 MPa @Strain 300 % |
319 psi @Strain 300 % |
ASTM D412 |
ExxonMobil Vistamaxx™ 6102 Propylene-based Elastomer Product Description: Vistamaxx 6102 propylene-based elastomer is an olefinic elastomer produced using ExxonMobil Chemical's EXXPOL™ Catalyst Technology. It has excellent elastomeric properties, i.. |
|||
Tensile Stress | 2.20 MPa @Strain 300 % |
319 psi @Strain 300 % |
ASTM D412 |
ExxonMobil Vistamaxx™ 6102FL Propylene-based Elastomer - Performance Film Product Description: Vistamaxx 6102FL propylene-based elastomer is an olefinic elastomer primarily composed of isostatic propylene repeat units with random ethylene distribution. It is produced us.. |
|||
Tensile Stress | 2.20 MPa @Strain 6.30 %, Temperature 60.0 °C |
319 psi @Strain 6.30 %, Temperature 140 °F |
TPE; ISO 11403-1 -2 |
DuPont Performance Polymers Hytrel® G4074 Polyester Elastomer TPC-ET
(Unverified Data**) 40 Shore D Standard Performance Polyester Elastomer with Heat Ageing ProtectionHytrel G4074 is a low modulus grade with nominal hardness of 40D. It contains discoloring stabilizer. It can be process.. |
|||
Tensile Stress | 2.20 MPa @Strain 8.92 %, Temperature 90.0 °C |
319 psi @Strain 8.92 %, Temperature 194 °F |
ISO 527 |
DuPont Performance Polymers Hytrel® G4078W TPC-ET
(Unverified Data**) Hytrel® G4078W is a low modulus grade with nominal hardness of 40D. It contains non-discoloring stabilizer. It can be processed by many conventional thermoplastic processing techniques like inject.. |
|||
Tensile Stress | 2.20 MPa @Strain 100 % |
319 psi @Strain 100 % |
ISO 37 |
Alliance Polymers Viprene™ G65A-32U-BLK Thermoplastic Vulcanizate Elastomer Viprene™ G65A-32U-BLK is a UV and Heat Stabilized TVP (Thermoplastic Vulcanizate Elastomer). This material can be easily processed by extrusion or injection molding. It exhibits easy flowing charac.. |
|||
Tensile Stress | 2.20 MPa @Strain 100 % |
319 psi @Strain 100 % |
ISO 37 |
Alliance Polymers Viprene™ G65A-32U-NAT Thermoplastic Vulcanizate Elastomer Viprene™ G65A-32U-NAT is a UV and Heat Stabilized TVP (Thermoplastic Vulcanizate Elastomer). This material can be easily processed by extrusion or injection molding. It exhibits easy flowing charac.. |
|||
Tensile Stress | 2.20 MPa @Strain 100 % |
319 psi @Strain 100 % |
ISO 37 |
Alliance Polymers Viprene™ P60A-22U-BLK Thermoplastic Vulcanizate Elastomer Viprene™ P60A-22U-BLK is a UV and Heat Stabilized TVP (Thermoplastic Vulcanizate Elastomer). This material can be easily processed by extrusion or injection molding. It exhibits easy flowing charac.. |
|||
Tensile Stress | 2.20 MPa @Strain 100 % |
319 psi @Strain 100 % |
ISO 37 |
Alliance Polymers Viprene™ P60A-22U-NAT Thermoplastic Vulcanizate Elastomer Viprene™ P60A-22U-NAT is a UV and Heat Stabilized TVP (Thermoplastic Vulcanizate Elastomer). This material can be easily processed by extrusion or injection molding. It exhibits easy flowing charac.. |
|||
Tensile Stress | >= 2.20 MPa @Strain 100 % |
>= 319 psi @Strain 100 % |
ISO 37 |
Austin Novel Materials Texalan® 370A Polyester-based TPU Description: Good abrasion resistance, tensile strength, oil resistance which can be used in injection, extrusion purpose.Information from Dawnentech |
|||
Tensile Stress | 2.20 MPa @Strain 0.100 %, Temperature 23.0 °C |
319 psi @Strain 0.100 %, Temperature 73.4 °F |
50%RH; ISO 11403-1 -2 |
DuPont Performance Polymers Minlon® 12T NC010 Nylon 66
(Unverified Data**) 36% Mineral Reinforced Toughened Polyamide 66 Minlon 12T NC010 is a 36% mineral reinforced toughened heat stabilized polyamide 66 resin for injection molding.Information provided by DuPont Performan.. |