Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

ExxonMobil Vistamaxx™ 6202FL Propylene-based Elastomer - Performance Film

Category Polymer , Film , Thermoplastic , Elastomer, TPE , Thermoplastic Olefinic Elastomer (TPO), Film Grade
Manufacturer Exxon Chemical
Trade Name Vistamaxx™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF ExxonMobil Vistamaxx™ 6202FL Propylene-based Elastomer - Performance Film.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Product Description: Vistamaxx 6202FL propylene-based elastomer is an olefinic elastomer primarily composed of isostatic propylene repeat units with random ethylene distribution, and is produced using ExxonMobil Chemical's EXXPOL™ Catalyst Technology. The "FL" designates this product passes ExxonMobil Chemical's test for film appearance with regard to gels, as needed for performance film applications ('A' rating).Key Features:Suitable for a wide range of cast film, extrusion coating, extrusion lamination and injection molding applications.Very good elasticity, flexibility and toughness.Compatible with a broad range array of materials and particularly good for polyolefinic and thermoplastic blends, including with styrenic block copolymersExcellent adhesion to conventional and metallocene PP and PE, and to various polyolefinic substrates (film, woven and nonwoven).Very low seal initiation temperature combined with high seal strength when used as an extrusion coating or laminating layer.High peel forces when used as adhesive layer of co-extruded surface protection films and masking tapes.Very effective at increasing to coefficient of friction of PE or PP blends.Good chemical resistance to aqueous systems and non-hydrocarbon based fluids.May be used in food contact applications (with some restrictions).EU and China RoHS compliant.Applications:Calendered ProfilesExtruded profilesExtrusion LaminationCalendered SheetingExtruded SheetingInjection MoldingCast FilmExtrusion CoatingPP/TPE ModificationUses:CompoundingFilmPackaging Availability: Africa & Middle East, Europe, North America, Asia Pacific, Latin America and South AmericaInformation provided by ExxonMobil Chemical.
Physical Properties Metric English Comments
Specific Gravity 0.863 g/cc
0.863 g/cc
ASTM D1505
Melt Flow 20 g/10 min
20 g/10 min
melt flow rate; ExxonMobil Method
9.1 g/10 min

@Load 2.16 kg,
Temperature 190 °C
9.1 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ExxonMobil Method
Mechanical Properties Metric English Comments
Hardness, Shore A 66

@Time 15.0 sec
66

@Time 0.00417 hour
ISO 868
Tensile Stress 1.90 MPa

@Strain 100 %
276 psi

@Strain 100 %
ASTM D412
2.10 MPa

@Strain 300 %
305 psi

@Strain 300 %
ASTM D412
Flexural Modulus, 1% Secant 12.3 MPa
1780 psi
ASTM D790
Tear Strength 33.3 kN/m
190 pli
Die C; ASTM D624
Tensile Set 18 %
18 %
ASTM D412
Thermal Properties Metric English Comments
Vicat Softening Point 47.1 °C
117 °F
ASTM D1525
Descriptive Properties Value Comments
Ethylene Content 15.0 wt%
ASTM D3900