Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Stress 3.67 MPa

@Strain 14.98 %,
Temperature 60.0 °C
532 psi

@Strain 14.98 %,
Temperature 140 °F
TPE; ISO 11403-1 -2
DuPont Performance Polymers Hytrel® 4056 Polyester Elastomer TPC-ET  (Unverified Data**)
40 Shore D High Performance Polyester ElastomerInformation provided by DuPont Performance Polymers
Tensile Stress 3.67 MPa

@Strain 147.33 %,
Temperature 120 °C
532 psi

@Strain 147.33 %,
Temperature 248 °F
TPE; ISO 11403-1 -2
DuPont Performance Polymers Hytrel® 4068FG Polyester Elastomer TPC-ET  (Unverified Data**)
40 Shore D High Performance Polyester Elastomer Developed for Food Contact ApplicationsInformation provided by DuPont Performance Polymers
Tensile Stress 3.67 MPa

@Strain 5.61 %,
Temperature 40.0 °C
532 psi

@Strain 5.61 %,
Temperature 104 °F
TPE; ISO 11403-1 -2
DuPont Performance Polymers Hytrel® HTR8139BK Polyester Elastomer TPC-ET  (Unverified Data**)
44 Shore D Lubricated High Viscosity Polyester Elastomer Developed for Blow Molding Hytrel HTR8139BK is designed for blow molding or processing techniques requiring high melt viscosity. It has nomin..
Tensile Stress 3.67 MPa

@Strain 14.49 %,
Temperature 120 °C
532 psi

@Strain 14.49 %,
Temperature 248 °F
TPE; ISO 11403-1 -2
DuPont Performance Polymers Hytrel® HTR8223 BK320 Polyester Elastomer TPC-ET  (Unverified Data**)
42 Shore D High Viscosity Polyester Elastomer Developed for Blow MoldingInformation provided by DuPont Performance Polymers