Polymer Property : Tensile Stress = 3.08 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Stress 3.08 MPa

@Strain 300 %
446 psi

@Strain 300 %
ASTM D412
Polymax® Maxelast® A9750 TPE, ABS/PC Overmold
Polymax's TPE material complies with UL, VDE, FDA, RoHS and PAH's standards.Uses:Consumer ProductsToys & NoveltiesAuto PartsTool Hand GripsSporting GoodsWire & Cable ElectronicsMedical DevicesInform..
Tensile Stress 3.08 MPa

@Strain 100 %
447 psi

@Strain 100 %
ASTM D412
Polymax® Maxelast® F02-087A TPE, Halogen Free Extrusion Grade
Characteristics: Good melt strengthSoft touchSmooth surface with dry feelGood weather and heat resistanceWide range of hardnessEasy processing Halogen FreeLow smoke emissionRoHs compliantDesigned to..
Tensile Stress 3.08 MPa

@Strain 300 %
447 psi

@Strain 300 %
ASTM D412
Polymax® Maxelast® P2945T TPE, PP Overmold or Standalone use
Polymax's TPE material complies with UL, VDE, FDA, RoHS and PAH's standards.Uses:Consumer ProductsToys & NoveltiesAuto PartsTool Hand GripsSporting GoodsWire & Cable ElectronicsMedical DevicesPlasti..
Tensile Stress 3.08 MPa

@Strain 100 %
446 psi

@Strain 100 %
NEU NeuSoft™ 596-60A Medical Ether TPU / SBC blend
Tensile Stress 3.08 MPa

@Strain 31.86 %,
Temperature 100 °C
447 psi

@Strain 31.86 %,
Temperature 212 °F
TPE; ISO 11403-1 -2
DuPont Performance Polymers Hytrel® 4056 Polyester Elastomer TPC-ET  (Unverified Data**)
40 Shore D High Performance Polyester ElastomerInformation provided by DuPont Performance Polymers
Tensile Stress 3.08 MPa

@Strain 46.89 %,
Temperature 60.0 °C
447 psi

@Strain 46.89 %,
Temperature 140 °F
TPE; ISO 11403-1 -2
DuPont Performance Polymers Hytrel® 3078FG Polyester Elastomer TPC-ET  (Unverified Data**)
30 Shore D High Performance Polyester Elastomer Developed for Food Contact ApplicationsInformation provided by DuPont Performance Polymers