Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Tensile Stress = 2970 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Stress 20.5 MPa

@Strain 0.360 %,
Temperature 23.0 °C
2970 psi

@Strain 0.360 %,
Temperature 73.4 °F
ISO 11403-1 -2
DuPont Performance Polymers Crastin® HR5315HF NC010 Polybutylene Terephthalate (PBT)  (Unverified Data**)&
15% Glass Reinforced Hydrolysis Resistant Polybutylene Terephthalate Crastin HR5315HF is a 15% glass reinforced PBT with high flow (HF) moderately toughened hydrolysis resistant (HR) resin. Excellen..
Tensile Stress 20.5 MPa

@Strain 1.70 %,
Temperature 90.0 °C
2970 psi

@Strain 1.70 %,
Temperature 194 °F
ISO 11403-1 -2
DuPont Performance Polymers Delrin® 500PE BK602 Acetal (POM)  (Unverified Data**)
Medium Viscosity Acetal Homopolymer with Very Low Emissions Delrin 500PE BK602 (formerly DE20578) is a medium viscosity acetal homopolymer an enhanced version of Delrin 500P with very low VOC emissi..
Tensile Stress 20.5 MPa

@Strain 30.0 %,
Temperature 0.000 °C
2970 psi

@Strain 30.0 %,
Temperature 32.0 °F
ISO 527
DuPont Performance Polymers Hytrel® DYM500BK TPC-ET  (Unverified Data**)
Hytrel® DYM500BK is a medium modulus polyester alloy suited for injection molding of Air Bag Deployment Doors. It has a nominal durometer hardness of 55D and contains fine particle size carbon blac..
Tensile Stress 20.5 MPa

@Strain 1.05 %,
Temperature 150 °C
2970 psi

@Strain 1.05 %,
Temperature 302 °F
ISO 527
DuPont Performance Polymers Rynite® 408 NC010 PET
Rynite® 408 NC010 is a 30% glass reinforced modified polyethylene terephthalate with improved impact resistance. Excellent balance of strength, stiffness, toughness, and temperature resistance.Inf..
Tensile Stress 20.5 MPa

@Strain 0.520 %,
Temperature 60.0 °C
2970 psi

@Strain 0.520 %,
Temperature 140 °F
50%RH; ISO 527
DuPont Performance Polymers Zytel® 70G20HSL NC010 Nylon 66
Information provided by DuPont Performance Polymers
Copyright © lookpolymers.com All Rights Reserved