Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 20.5 MPa @Strain 0.360 %, Temperature 23.0 °C |
2970 psi @Strain 0.360 %, Temperature 73.4 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Crastin® HR5315HF NC010 Polybutylene Terephthalate (PBT)
(Unverified Data**)& 15% Glass Reinforced Hydrolysis Resistant Polybutylene Terephthalate Crastin HR5315HF is a 15% glass reinforced PBT with high flow (HF) moderately toughened hydrolysis resistant (HR) resin. Excellen.. |
|||
Tensile Stress | 20.5 MPa @Strain 1.70 %, Temperature 90.0 °C |
2970 psi @Strain 1.70 %, Temperature 194 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Delrin® 500PE BK602 Acetal (POM)
(Unverified Data**) Medium Viscosity Acetal Homopolymer with Very Low Emissions Delrin 500PE BK602 (formerly DE20578) is a medium viscosity acetal homopolymer an enhanced version of Delrin 500P with very low VOC emissi.. |
|||
Tensile Stress | 20.5 MPa @Strain 30.0 %, Temperature 0.000 °C |
2970 psi @Strain 30.0 %, Temperature 32.0 °F |
ISO 527 |
DuPont Performance Polymers Hytrel® DYM500BK TPC-ET
(Unverified Data**) Hytrel® DYM500BK is a medium modulus polyester alloy suited for injection molding of Air Bag Deployment Doors. It has a nominal durometer hardness of 55D and contains fine particle size carbon blac.. |
|||
Tensile Stress | 20.5 MPa @Strain 1.05 %, Temperature 150 °C |
2970 psi @Strain 1.05 %, Temperature 302 °F |
ISO 527 |
DuPont Performance Polymers Rynite® 408 NC010 PET Rynite® 408 NC010 is a 30% glass reinforced modified polyethylene terephthalate with improved impact resistance. Excellent balance of strength, stiffness, toughness, and temperature resistance.Inf.. |
|||
Tensile Stress | 20.5 MPa @Strain 0.520 %, Temperature 60.0 °C |
2970 psi @Strain 0.520 %, Temperature 140 °F |
50%RH; ISO 527 |
DuPont Performance Polymers Zytel® 70G20HSL NC010 Nylon 66 Information provided by DuPont Performance Polymers |