Polymer Property : Tensile Stress = 276 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Stress 1.90 MPa

@Strain 300 %
276 psi

@Strain 300 %
Across Flow; ISO 37
PolyOne OnFlex™ HT 50A-3S2099 Thermoplastic Elastomer (TPE)
OnFlex™ HT thermoplastic elastomer compounds are based on hydrogenated styrenic block copolymers. This range of compounds is specially formulated to deliver very good compression set performance at..
Tensile Stress 1.90 MPa

@Strain 300 %
276 psi

@Strain 300 %
ISO 37
PolyOne OnFlex™ S EF 40A-3S1964 Thermoplastic Elastomer (TPE)
OnFlex™-S EF thermoplastic elastomer compounds are based on hydrogenated styrenic block copolymers. This range of compounds are formulated to deliver good mechanical properties together with excell..
Tensile Stress 1.90 MPa

@Strain 100 %
276 psi

@Strain 100 %
ISO 37
PolyOne OnFlex™ S EF 60A-3S1967 Thermoplastic Elastomer (TPE)
OnFlex™-S EF thermoplastic elastomer compounds are based on hydrogenated styrenic block copolymers. This range of compounds are formulated to deliver good mechanical properties together with excell..
Tensile Stress 1.90 MPa

@Strain 300 %
276 psi

@Strain 300 %
ISO 37
PolyOne OnFlex™ S FR 25A-3S1830 Thermoplastic Elastomer (TPE)
OnFlex™-S FR thermoplastic elastomer compounds are based on hydrogenated styrenic block copolymers. This range of compounds are specially flame retarded with a highly effective, RoHS compliant halo..
Tensile Stress 1.90 MPa

@Strain 100 %,
Temperature 23.0 °C
276 psi

@Strain 100 %,
Temperature 73.4 °F
Die C2 hr; ASTM D412
PolyOne Versaflex™ OM 6258-1 Thermoplastic Elastomer (TPE)
Versaflex™ OM 6258-1 is specifically designed to bond to a variety of standard and modified nylon materials, including those which are glass-filled, heat stabilized and/or impact modified. - Except..
Tensile Stress 1.90 MPa

@Strain 100 %,
Temperature 23.0 °C
276 psi

@Strain 100 %,
Temperature 73.4 °F
Die C2 hr; ASTM D412
PolyOne Versaflex™ OM 6258-9 Thermoplastic Elastomer (TPE)
Versaflex™ OM 6258-9 is specifically designed to bond to a variety of standard and modified nylon materials, including those which are glass-filled, heat stabilized and/or impact modified. - Except..
Tensile Stress 1.90 MPa

@Strain 100 %
276 psi

@Strain 100 %
ASTM D412
Polymax® Maxelast® P3865A TPE, PP Overmold or Standalone use
Polymax's TPE material complies with UL, VDE, FDA, RoHS and PAH's standards.Uses:Consumer ProductsToys & NoveltiesAuto PartsTool Hand GripsSporting GoodsWire & Cable ElectronicsMedical DevicesPlasti..
Tensile Stress 1.90 MPa

@Strain 300 %,
Temperature 23.0 °C
276 psi

@Strain 300 %,
Temperature 73.4 °F
Die C2 hr; ASTM D412
PolyOne Dynalloy™ OBC 8100-N50 Thermoplastic Elastomer (TPE)
Dynalloy™ OBC8100-N50 is a TPE developed utilizing the unique rubber properties of Dow INFUSE™ Olefin Block Copolymers. The 8100 Series has been specifically developed for applications requiring t..
Tensile Stress 1.90 MPa

@Strain 10.0 %
276 psi

@Strain 10.0 %
ISO 527-1/-2
DSM Arnitel® XG5858 TPC-ET
Injection Molding
Tensile Stress 1.90 MPa

@Strain 100 %
276 psi

@Strain 100 %
ASTM D412
ExxonMobil Vistamaxx™ 6102 Propylene-based Elastomer
Product Description: Vistamaxx 6102 propylene-based elastomer is an olefinic elastomer produced using ExxonMobil Chemical's EXXPOL™ Catalyst Technology. It has excellent elastomeric properties, i..
Tensile Stress 1.90 MPa

@Strain 100 %
276 psi

@Strain 100 %
ASTM D412
ExxonMobil Vistamaxx™ 6102FL Propylene-based Elastomer - Performance Film
Product Description: Vistamaxx 6102FL propylene-based elastomer is an olefinic elastomer primarily composed of isostatic propylene repeat units with random ethylene distribution. It is produced us..
Tensile Stress 1.90 MPa

@Strain 100 %
276 psi

@Strain 100 %
ASTM D412
ExxonMobil Vistamaxx™ 6202 Propylene-based Elastomer
Product Description: Vistamaxx 6202 propylene-based elastomer is an olefinic elastomer produced using ExxonMobil Chemical's EXXPOL™ Catalyst Technology. It has excellent elastomeric properties, i..
Tensile Stress 1.90 MPa

@Strain 100 %
276 psi

@Strain 100 %
ASTM D412
ExxonMobil Vistamaxx™ 6202FL Propylene-based Elastomer - Performance Film
Product Description: Vistamaxx 6202FL propylene-based elastomer is an olefinic elastomer primarily composed of isostatic propylene repeat units with random ethylene distribution, and is produced us..
Tensile Stress 1.90 MPa

@Strain 100 %
276 psi

@Strain 100 %
ISO 37
Alliance Polymers Viprene™ G55A-32U-BLK Thermoplastic Vulcanizate Elastomer
Viprene™ G55A-32U-BLK is a UV and Heat Stabilized TVP (Thermoplastic Vulcanizate Elastomer). This material can be easily processed by extrusion or injection molding. It exhibits easy flowing charac..
Tensile Stress 1.90 MPa

@Strain 100 %
276 psi

@Strain 100 %
ISO 37
Alliance Polymers Viprene™ G55A-32U-NAT Thermoplastic Vulcanizate Elastomer
Viprene™ G55A-32U-NAT is a UV and Heat Stabilized TVP (Thermoplastic Vulcanizate Elastomer). This material can be easily processed by extrusion or injection molding. It exhibits easy flowing charac..