Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 16.22 MPa @Strain 0.260 %, Temperature 40.0 °C |
2353 psi @Strain 0.260 %, Temperature 104 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Crastin® LW9020FR NC010 PBT+ASA
(Unverified Data**) 20% Glass Reinforced Flame Retardant Polybutylene Terephthalate Blend with Low Warpage Characteristics Crastin LW9020FR NC010 is a 20% glass fiber reinforced flame retardant polybutylene terephthal.. |