Polymer Property : Tensile Stress = 16.22 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Stress 16.22 MPa

@Strain 0.260 %,
Temperature 40.0 °C
2353 psi

@Strain 0.260 %,
Temperature 104 °F
ISO 11403-1 -2
DuPont Performance Polymers Crastin® LW9020FR NC010 PBT+ASA  (Unverified Data**)
20% Glass Reinforced Flame Retardant Polybutylene Terephthalate Blend with Low Warpage Characteristics Crastin LW9020FR NC010 is a 20% glass fiber reinforced flame retardant polybutylene terephthal..