Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 15.5 MPa @Strain 100 % |
2250 psi @Strain 100 % |
ISO 527-1/-2 |
DSM Arnitel® PM460-H TPC-ET Injection Molding, Heat Stabilized |
|||
Tensile Stress | 15.5 MPa @Strain 1.48 %, Temperature 150 °C |
2250 psi @Strain 1.48 %, Temperature 302 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Crastin® LW9030FR NC010 PBT+ASA
(Unverified Data**) 30% Glass Reinforced Flame Retardant Polybutylene Terephthalate Blend with Low Warpage Characteristics Crastin LW9030FR NC010 is a 30% glass fiber reinforced flame retardant polybutylene terephthal.. |
|||
Tensile Stress | 15.5 MPa @Strain 2.00 %, Temperature 40.0 °C |
2250 psi @Strain 2.00 %, Temperature 104 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Delrin® 100ST NC010 Acetal (POM)
(Unverified Data**) Super Toughened High Viscosity Acetal Homopolymer Delrin 100ST NC010 is a super tough high viscosity acetal homopolymer grade with superior impact resistance. It is designed for highly stressed part.. |
|||
Tensile Stress | 15.5 MPa @Strain 7.03 %, Temperature 60.0 °C |
2250 psi @Strain 7.03 %, Temperature 140 °F |
TPE; ISO 11403-1 -2 |
DuPont Performance Polymers Hytrel® 8238 Polyester Elastomer TPC-ET
(Unverified Data**) 82 Shore D Standard Performance Polyester ElastomerInformation provided by DuPont Performance Polymers |
|||
Tensile Stress | 15.5 MPa @Strain 1.50 %, Temperature 160 °C |
2250 psi @Strain 1.50 %, Temperature 320 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Crastin® SK641FR NC010 Polybutylene Terephthalate (PBT) 10% Glass Reinforced Flame Retardant Polybutylene Terephthalate Information provided by DuPont Performance Polymers |