Tensile Stress 15.5 MPa

@Strain 100 %
2250 psi

@Strain 100 %
ISO 527-1/-2
DSM Arnitel® PM460-H TPC-ET
Injection Molding, Heat Stabilized
Tensile Stress 15.5 MPa

@Strain 1.48 %,
Temperature 150 °C
2250 psi

@Strain 1.48 %,
Temperature 302 °F
ISO 11403-1 -2
DuPont Performance Polymers Crastin® LW9030FR NC010 PBT+ASA  (Unverified Data**)
30% Glass Reinforced Flame Retardant Polybutylene Terephthalate Blend with Low Warpage Characteristics Crastin LW9030FR NC010 is a 30% glass fiber reinforced flame retardant polybutylene terephthal..
Tensile Stress 15.5 MPa

@Strain 2.00 %,
Temperature 40.0 °C
2250 psi

@Strain 2.00 %,
Temperature 104 °F
ISO 11403-1 -2
DuPont Performance Polymers Delrin® 100ST NC010 Acetal (POM)  (Unverified Data**)
Super Toughened High Viscosity Acetal Homopolymer Delrin 100ST NC010 is a super tough high viscosity acetal homopolymer grade with superior impact resistance. It is designed for highly stressed part..
Tensile Stress 15.5 MPa

@Strain 7.03 %,
Temperature 60.0 °C
2250 psi

@Strain 7.03 %,
Temperature 140 °F
TPE; ISO 11403-1 -2
DuPont Performance Polymers Hytrel® 8238 Polyester Elastomer TPC-ET  (Unverified Data**)
82 Shore D Standard Performance Polyester ElastomerInformation provided by DuPont Performance Polymers
Tensile Stress 15.5 MPa

@Strain 1.50 %,
Temperature 160 °C
2250 psi

@Strain 1.50 %,
Temperature 320 °F
ISO 11403-1 -2
DuPont Performance Polymers Crastin® SK641FR NC010 Polybutylene Terephthalate (PBT)
10% Glass Reinforced Flame Retardant Polybutylene Terephthalate Information provided by DuPont Performance Polymers
Copyright © lookpolymers.com All Rights Reserved