Polymer Property : Tensile Stress = 21800 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Stress 150 MPa

@Strain 3.00 %,
Temperature 0.000 °C
21800 psi

@Strain 3.00 %,
Temperature 32.0 °F
Solvay TECHNYL® A 218 V30 BK 34 NG PA66, 30% glass fiber, Conditioned
Description: TECHNYL® A 218 V30 Black 34 NG is a polyamide 66, reinforced with 30% of glass fiber, heat stabilized, for injection molding. The product is available in black color.Benefits: This p..
Tensile Stress 150 MPa

@Strain 4.00 %,
Temperature 60.0 °C
21800 psi

@Strain 4.00 %,
Temperature 140 °F
Solvay TECHNYL® A 218 V35 PA66, 35% glass fiber, DRY
Description: TECHNYL® A 218 V35 is a polyamide 66, reinforced with 35% of glass fiber, heat stabilized, for injection molding. This product is available in natural and black colors.Benefits: The ..
Tensile Stress 150 MPa

@Strain 5.00 %,
Temperature 60.0 °C
21800 psi

@Strain 5.00 %,
Temperature 140 °F
Solvay TECHNYL® A 218 V35 PA66, 35% glass fiber, DRY
Description: TECHNYL® A 218 V35 is a polyamide 66, reinforced with 35% of glass fiber, heat stabilized, for injection molding. This product is available in natural and black colors.Benefits: The ..
Tensile Stress 150 MPa

@Strain 1.00 %,
Temperature 23.0 °C
21800 psi

@Strain 1.00 %,
Temperature 73.4 °F
Solvay TECHNYL® A 218HP V50 PA66, 35% glass fiber, DRY
Description: TECHNYL® A 218HP V50 is a polyamide 66, reinforced with 50% of glass fiber, heat stabilized, for injection molding. This product is available in black color.Benefits: The product off..
Tensile Stress 150 MPa

@Strain 3.00 %,
Temperature 60.0 °C
21800 psi

@Strain 3.00 %,
Temperature 140 °F
Solvay TECHNYLSTARâ„¢ AFX 218 V60 PA6, 60% glass filled, Conditioned
Description: TECHNYLSTARâ„¢ AFX 218 V60 is based on a patented high flow polyamide 66 resin (Technylstar), heat stabilized, reinforced with 60% of glass fiber, for injection molding.Benefits: Due..
Tensile Stress 150 MPa

@Strain 2.00 %,
Temperature 80.0 °C
21800 psi

@Strain 2.00 %,
Temperature 176 °F
Solvay TECHNYLSTARâ„¢ AFX 218 V60 PA6, 60% glass filled, DRY
Description: TECHNYLSTARâ„¢ AFX 218 V60 is based on a patented high flow polyamide 66 resin (Technylstar), heat stabilized, reinforced with 60% of glass fiber, for injection molding.Benefits: Due..
Tensile Stress 150 MPa

@Strain 1.76 %,
Temperature -20.0 °C
21800 psi

@Strain 1.76 %,
Temperature -4.00 °F
DAM; ISO 11403-1 -2
DuPont Performance Polymers Minlon® EFE6053 BK413 Nylon 66  (Unverified Data**)
40% Mineral/Glass Reinforced Polyamide 66 Minlon EFE6053 BK413 is a 40% mineral/glass reinforced heat stabilized polyamide 66 resin for injection molding.Information provided by DuPont Performance P..
Tensile Stress 150 MPa

@Temperature 23.0 °C
21800 psi

@Temperature 73.4 °F
BASF Ultramid® Endure D3G7 Glass-Fiber Reinforced Polyamide
Description: Ultramid® Endure is a new, glass-fiber reinforced polyamide that combines excellent heat aging resistance with the good processing properties of PA 66. Ultramid® Endure can withstand ..
Tensile Stress 150 MPa

@Strain 2.00 %
21800 psi

@Strain 2.00 %
Solvay TECHNYL® A 20 V25 PA66, 25% glass fiber, DRY
Description: TECHNYL® A 20 V25 is a 25% glass fiber reinforced Red Phosphorous flame retarded grade based on a polyamide 66 resin. This product is heat stabiised for optimised injection moulding. T..
Tensile Stress 150 MPa

@Strain 2.73 %,
Temperature 40.0 °C
21800 psi

@Strain 2.73 %,
Temperature 104 °F
DAM; ISO 11403-1 -2
DuPont Performance Polymers Zytel® 70G25HSL NC010 Nylon 66  (Unverified Data**)
25% Glass Reinforced Heat Stabilized Polyamide 66 Zytel 70G25HSL NC010 is a 25% glass fiber reinforced heat stabilized polyamide 66 resin for injection molding.Information provided by DuPont Perform..
Copyright © lookpolymers.com All Rights Reserved