Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 148.97 MPa @Strain 1.46 %, Temperature -20.0 °C |
21606 psi @Strain 1.46 %, Temperature -4.00 °F |
DAM; ISO 11403-1/-2 |
DuPont Performance Polymers Zytel® 70G35HSLRA4 BK267 Nylon 66
(Unverified Data**) Zytel® 70G35HSLRA4 BK267 is a 35% glass fiber reinforced, heat stabilized, hydrolysis resistant polyamide 66 resin for injection molding. It has excellent flow characteristics.Information provided .. |
|||
Tensile Stress | 148.97 MPa @Strain 5.04 %, Temperature 40.0 °C |
21606 psi @Strain 5.04 %, Temperature 104 °F |
50%RH; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® PLS 95G50DH2 BK261 Nylon 6
(Unverified Data**) 50% Glass Reinforced Heat Stabilized Polyamide Zytel PLS95G50DH2 BK261is a high flow 50% glass reinforced PA nylon resin using SHIELD Technology only from DuPont providing exceptional Heat Resistanc.. |