Tensile Stress 148.97 MPa

@Strain 1.46 %,
Temperature -20.0 °C
21606 psi

@Strain 1.46 %,
Temperature -4.00 °F
DAM; ISO 11403-1/-2
DuPont Performance Polymers Zytel® 70G35HSLRA4 BK267 Nylon 66  (Unverified Data**)
Zytel® 70G35HSLRA4 BK267 is a 35% glass fiber reinforced, heat stabilized, hydrolysis resistant polyamide 66 resin for injection molding. It has excellent flow characteristics.Information provided ..
Tensile Stress 148.97 MPa

@Strain 5.04 %,
Temperature 40.0 °C
21606 psi

@Strain 5.04 %,
Temperature 104 °F
50%RH; ISO 11403-1 -2
DuPont Performance Polymers Zytel® PLS 95G50DH2 BK261 Nylon 6  (Unverified Data**)
50% Glass Reinforced Heat Stabilized Polyamide Zytel PLS95G50DH2 BK261is a high flow 50% glass reinforced PA nylon resin using SHIELD Technology only from DuPont providing exceptional Heat Resistanc..