Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 21.6 MPa @Strain 3.00 %, Temperature 160 °C |
3130 psi @Strain 3.00 %, Temperature 320 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Crastin® SK601 NC010 Polybutylene Terephthalate (PBT)
(Unverified Data**) 10% Glass Reinforced Polybutylene Terephthalate Crastin SK601 NC010 is a 10% glass fiber reinforced lubricated polybutylene terephthalate resin for injection molding.Information provided by DuPont P.. |
|||
Tensile Stress | 21.6 MPa @Strain 0.300 %, Temperature 23.0 °C |
3130 psi @Strain 0.300 %, Temperature 73.4 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Crastin® SK603 NC010 Polybutylene Terephthalate (PBT)
(Unverified Data**) 20% Glass Reinforced Polybutylene Terephthalate Crastin SK603 NC010 is a 20% glass fiber reinforced lubricated polybutylene terephthalate resin for injection molding.Information provided by DuPont P.. |
|||
Tensile Stress | 21.6 MPa @Strain 1.59 %, Temperature 120 °C |
3130 psi @Strain 1.59 %, Temperature 248 °F |
DAM; ISO 11403-1/-2 |
DuPont Performance Polymers Crastin® HR5315HF NC010 PBT
(Unverified Data**) Crastin® HR5315HF is a 15% glass reinforced PBT with high flow (HF), moderately toughened, hydrolysis resistant (HR) resin. Excellent balance of properties between terminal pullout and impact resis.. |