Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 1.41 MPa @Strain 300 % |
205 psi @Strain 300 % |
ASTM D412 |
Polymax® Maxelast® P3936C TPE, PP Overmold or Standalone use Polymax's TPE material complies with UL, VDE, FDA, RoHS and PAH's standards.Uses:Consumer ProductsToys & NoveltiesAuto PartsTool Hand GripsSporting GoodsWire & Cable ElectronicsMedical DevicesPlasti.. |
|||
Tensile Stress | 1.41 MPa @Strain 100 % |
205 psi @Strain 100 % |
ASTM D412 |
Teknor Apex Monprene® MP-2815C Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Tensile Stress | 1.41 MPa @Strain 19.13 %, Temperature 100 °C |
205 psi @Strain 19.13 %, Temperature 212 °F |
TPE; ISO 11403-1 -2 |
DuPont Performance Polymers Hytrel® 3078 Polyester Elastomer TPC-ET
(Unverified Data**) 30 Shore D High Performance Polyester Elastomer with Non-discoloring Stabilizer Hytrel 3078 is a very low modulus grade with nominal hardness of 30D. It contains non-discoloring stabilizer. It can b.. |
|||
Tensile Stress | 1.41 MPa @Strain 0.000 %, Temperature 120 °C |
205 psi @Strain 0.000 %, Temperature 248 °F |
50%RH; ISO 11403-1/-2 |
DuPont Performance Polymers Zytel® PLUS PLS95G50DH2 BK261 Nylon
(Unverified Data**) Zytel® PLS95G50DH2 BK261is a high flow 50% glass reinforced PA nylon resin using SHIELD Technology, only from DuPont providing exceptional Heat Resistance & High stiffness for automotive under hood.. |
|||
Tensile Stress | 1.41 MPa @Strain 19.13 %, Temperature 100 °C |
205 psi @Strain 19.13 %, Temperature 212 °F |
TPE; ISO 11403-1 -2 |
DuPont Performance Polymers Hytrel® 3078FG Polyester Elastomer TPC-ET
(Unverified Data**) 30 Shore D High Performance Polyester Elastomer Developed for Food Contact ApplicationsInformation provided by DuPont Performance Polymers |
|||
Tensile Stress | 1.41 MPa @Strain 1.50 %, Temperature 40.0 °C |
205 psi @Strain 1.50 %, Temperature 104 °F |
TPE; ISO 11403-1 -2 |
DuPont Performance Polymers Hytrel® HTR8341C BK320 Polyester Elastomer TPC-ET
(Unverified Data**) 40 Shore D Lubricated High Viscosity Polyester Elastomer with Superior Fatigue Resistance Developed for Blow Molding Information provided by DuPont Performance Polymers |