Mechanical Properties Metric English Comments
Tensile Stress 2.28 MPa

@Strain 100 %,
Temperature 23.0 °C
331 psi

@Strain 100 %,
Temperature 73.4 °F
Die C2 hr; ASTM D412
PolyOne Versaflex™ OM 6160-1 Thermoplastic Elastomer (TPE)
Versaflex™ OM 6160-1 is specifically designed to bond to a variety of standard and modified nylon materials, including those which are glass-filled, heat stabilized and/or impact modified. - Excell..
Tensile Stress 2.28 MPa

@Strain 100 %,
Temperature 23.0 °C
331 psi

@Strain 100 %,
Temperature 73.4 °F
Die C2 hr; ASTM D412
PolyOne Versaflex™ OM 6160-9 Thermoplastic Elastomer (TPE)
Versaflex™ OM 6160-9 is specifically designed to bond to a variety of standard and modified nylon materials, including those which are glass-filled, heat stabilized and/or impact modified. - Excell..
Tensile Stress 2.28 MPa

@Strain 300 %,
Temperature 23.0 °C
331 psi

@Strain 300 %,
Temperature 73.4 °F
Die C2 hr; ASTM D412
PolyOne Dynaflex™ G2755-1000-00 Thermoplastic Elastomer (TPE)
Dynaflex™ G2755-1000-00 is an easy processing TPE designed for injection molding and extrusion applications that require FDA compliance. - Good Ozone and UV Stability - Overmold Adhesion to Polypro..
Tensile Stress 2.28 MPa

@Strain 300 %
331 psi

@Strain 300 %
510 mm/min; ASTM D412A
PolyOne Elastamax™ HTE 1105 Styrene Butadiene Block Copolymer (SBC)
Information provided by PolyOne
Tensile Stress 2.28 MPa

@Strain 100 %
330 psi

@Strain 100 %
ASTM D412
Teknor Apex Telcar® TL-1050-75 Thermoplastic Elastomer
Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets P..
Tensile Stress 2.28 MPa

@Strain 100 %
330 psi

@Strain 100 %
ASTM D412
Teknor Apex Telcar® TL-91-T3056D-75 Thermoplastic Elastomer
Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets ..
Tensile Stress 2.28 MPa

@Strain 149.65 %,
Temperature 100 °C
331 psi

@Strain 149.65 %,
Temperature 212 °F
TPE; ISO 11403-1 -2
DuPont Performance Polymers Hytrel® 3078 Polyester Elastomer TPC-ET  (Unverified Data**)
30 Shore D High Performance Polyester Elastomer with Non-discoloring Stabilizer Hytrel 3078 is a very low modulus grade with nominal hardness of 30D. It contains non-discoloring stabilizer. It can b..
Tensile Stress 2.28 MPa

@Strain 0.100 %,
Temperature 40.0 °C
331 psi

@Strain 0.100 %,
Temperature 104 °F
50%RH; ISO 11403-1 -2
DuPont Performance Polymers Zytel® HTN FE8200 NC010 Polyphthalamide (PPA)  (Unverified Data**)
Unreinforced Toughened PPA High Performance Polyamide Zytel HTNFE8200 NC010 is an unreinforced toughened heat stabilized lubricated high performance polyamide resin for injection molding. It is also..
Tensile Stress 2.28 MPa

@Strain 149.65 %,
Temperature 100 °C
331 psi

@Strain 149.65 %,
Temperature 212 °F
TPE; ISO 11403-1 -2
DuPont Performance Polymers Hytrel® 3078FG Polyester Elastomer TPC-ET  (Unverified Data**)
30 Shore D High Performance Polyester Elastomer Developed for Food Contact ApplicationsInformation provided by DuPont Performance Polymers