Tensile Stress 2.28 MPa

@Strain 100 %
330 psi

@Strain 100 %
ASTM D412
Teknor Apex Telcar® TL-1050-75 Thermoplastic Elastomer
Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets P..
Tensile Stress 2.28 MPa

@Strain 100 %
330 psi

@Strain 100 %
ASTM D412
Teknor Apex Telcar® TL-91-T3056D-75 Thermoplastic Elastomer
Uses: Automotive Applications; Automotive Exterior Parts; Automotive Exterior Trim; Automotive Interior Parts; Blow Molding Applications; General Purpose; Grommets; Weatherstripping Forms: Pellets ..