Polymer Property : Tensile Stress = 19600 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Stress 135 MPa

@Strain 2.00 %,
Temperature 0.000 °C
19600 psi

@Strain 2.00 %,
Temperature 32.0 °F
Solvay TECHNYL® A 218 V30 BK 34 NG PA66, 30% glass fiber, Conditioned
Description: TECHNYL® A 218 V30 Black 34 NG is a polyamide 66, reinforced with 30% of glass fiber, heat stabilized, for injection molding. The product is available in black color.Benefits: This p..
Tensile Stress 135 MPa

@Strain 3.00 %,
Temperature 80.0 °C
19600 psi

@Strain 3.00 %,
Temperature 176 °F
Solvay TECHNYLSTARâ„¢ AFX 218 V60 PA6, 60% glass filled, Conditioned
Description: TECHNYLSTARâ„¢ AFX 218 V60 is based on a patented high flow polyamide 66 resin (Technylstar), heat stabilized, reinforced with 60% of glass fiber, for injection molding.Benefits: Due..
Tensile Stress 135 MPa

@Strain 2.00 %
19600 psi

@Strain 2.00 %
Solvay TECHNYLSTARâ„¢ S 60G1 V30 PA6, 30% glass filled, DRY
Description: TECHNYLSTARâ„¢ S 60G1 V30 is a reinforced 30% GF organophosphorous flame retarded grade based on a patented high flow polyamide 6 resin (TechnylStar). This product is heat stabilized..
Tensile Stress 135.14 MPa

@Strain 2.05 %,
Temperature 23.0 °C
19600 psi

@Strain 2.05 %,
Temperature 73.4 °F
DAM; ISO 11403-1 -2
DuPont Performance Polymers Zytel® RS 30G30L NC010 Nylon 610
30% Glass Reinforced Renewably Sourced Polyamide 610 Developed for Extrusion Zytel RS 30G30L NC010 is a lubricated 30% glass fiber reinforced polyamide 610 resin containing a minimum of 40% renewabl..
Tensile Stress 135 MPa

@Strain 1.00 %,
Temperature 60.0 °C
19600 psi

@Strain 1.00 %,
Temperature 140 °F
Akro-Plastic Akroloy® PA GF 50 (2706) PA 6.6 & PA6I/6T Dry, 50% Glass Filled
One of the most characteristic properties of polyamide (PA 6.6) is the absorption of moisture. This essentially leads to increased toughness and elongation at break, to name the most important param..
Tensile Stress 135 MPa

@Strain 3.00 %,
Temperature 80.0 °C
19600 psi

@Strain 3.00 %,
Temperature 176 °F
Akro-Plastic Akroloy® PA GF 50 (2706) PA 6.6 & PA6I/6T Dry, 50% Glass Filled
One of the most characteristic properties of polyamide (PA 6.6) is the absorption of moisture. This essentially leads to increased toughness and elongation at break, to name the most important param..
Tensile Stress 135 MPa

@Strain 0.810 %,
Temperature -40.0 °C
19600 psi

@Strain 0.810 %,
Temperature -40.0 °F
ISO 11403-1 -2
DuPont Performance Polymers Rynite® 545 NC010 Polyethylene Terephthalate (PET)  (Unverified Data**)
45% Glass Reinforced Polyethylene Terephthalate Rynite 545 NC010 is a 45% glass reinforced modified polyethylene terephthalate with greater strength and stiffness excellent dimensional stability and..