Mechanical Properties Metric English Comments
Tensile Stress 19.3 MPa

@Strain 6.52 %,
Temperature 90.0 °C
2800 psi

@Strain 6.52 %,
Temperature 194 °F
ISO 527
DuPont Performance Polymers Delrin® 100T NC010 Acetal Homopolymer  (Unverified Data**)
Delrin® 100T NC010 is a toughened, high viscosity acetal homopolymer grade with high impact resistance.Information provided by DuPont Performance Polymers
Tensile Stress 19.3 MPa

@Strain 100 %
2800 psi

@Strain 100 %
ASTM D412
Teknor Apex Uniprene® UN-7010-40D-NT Thermoplastic Vulcanizate
Notes: Injection Rate: Fast Uses: Gaskets; Glazing; Grommets; Medical Pump Seals; Medical/Healthcare Applications; Plugs; Shock Absorbing Pads; Tubing Agency Ratings: NSF 61 Forms: Pellets Processin..
Tensile Stress 19.3 MPa

@Strain 6.50 %,
Temperature 90.0 °C
2800 psi

@Strain 6.50 %,
Temperature 194 °F
ISO 11403-1 -2
DuPont Performance Polymers Delrin® 100T NC010 Acetal (POM)  (Unverified Data**)
Toughened High Viscosity Acetal Homopolymer Delrin 100T NC010 is a toughened high viscosity acetal homopolymer grade with high impact resistance.Information provided by DuPont Performance Polymers
Tensile Stress 19.3 MPa

@Strain 4.60 %,
Temperature 90.0 °C
2800 psi

@Strain 4.60 %,
Temperature 194 °F
DAM; ISO 11403-1 -2
DuPont Performance Polymers Zytel® 103HSL NC010 Nylon 66  (Unverified Data**)
Unreinforced Heat Stabilized Polyamide 66 Zytel 103HSL NC010 is a heat stabilized lubricated polyamide 66 resin for injection molding.Information provided by DuPont Performance Polymers
Tensile Stress 19.3 MPa

@Strain 0.250 %,
Temperature -20.0 °C
2800 psi

@Strain 0.250 %,
Temperature -4.00 °F
ISO 11403-1 -2
DuPont Performance Polymers Crastin® LW9020 NC010 PBT+ASA  (Unverified Data**)
20% Glass Reinforced Polybutylene Terephthalate Blend with Low Warpage Characteristics Crastin LW9020 NC010 is a 20% glass fiber reinforced polybutylene terephthalate blend for injection molding. ..