Polymer Property : Tensile Stress = 170 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Stress 170 MPa

@Strain 2.00 %,
Temperature -30.0 °C
24700 psi

@Strain 2.00 %,
Temperature -22.0 °F
Solvay TECHNYL® A 218 V30 PA66, 30% glass fiber, DRY
Description: TECHNYL® A 218 V30 is a polyamide 66, reinforced with 30% of glass fiber, heat stabilized, for injection molding. This product is available in natural and black colors.Benefits: The ..
Tensile Stress 170 MPa

@Strain 2.00 %,
Temperature 60.0 °C
24700 psi

@Strain 2.00 %,
Temperature 140 °F
Solvay TECHNYLSTARâ„¢ AFX 218 V60 PA6, 60% glass filled, DRY
Description: TECHNYLSTARâ„¢ AFX 218 V60 is based on a patented high flow polyamide 66 resin (Technylstar), heat stabilized, reinforced with 60% of glass fiber, for injection molding.Benefits: Due..
Tensile Stress 170 MPa

@Strain 3.00 %
24700 psi

@Strain 3.00 %
Solvay TECHNYLSTARâ„¢ S 218 V30 PA6, 30% glass filled, DRY
Description: TECHNYLSTARâ„¢ S 218 V30 is based on a patented high flow polyamide 6 resin (TechnylStar), heat stabilized, reinforced with 30% of glass fiber, for injection molding. This product is..
Tensile Stress 170 MPa

@Strain 0.300 %,
Temperature 982 °C
24700 psi

@Strain 0.300 %,
Temperature 1800 °F
COI Ceramics Sylramic™ S200 Silicon Carbide Ceramic Matrix Composite, CG Nicalon
Engineered ceramic composite structure.Reinforcing Fiber Flexibility: S400 - Carbon Preceramic Polymer Matrix Precursors: S400 - Crystalline (SiC + Si3N4) or SiCPhysical Attributes: Dense Matrix (
Tensile Stress 170 MPa

@Strain 4.00 %,
Temperature 120 °C
24700 psi

@Strain 4.00 %,
Temperature 248 °F
Akro-Plastic Akromid® T1 GF 50 (3101) PPA Dry, 50% Glass Filled
The new AKROMID® T is characterized primarily by high heat resistance and the lowest moisture absorption of the three PA grades, making it particularly well-suited in the automotive sector for high..
Tensile Stress 170 MPa

@Strain 2.50 %
24700 psi

@Strain 2.50 %
Solvay TECHNYL® A 20 V25 PA66, 25% glass fiber, DRY
Description: TECHNYL® A 20 V25 is a 25% glass fiber reinforced Red Phosphorous flame retarded grade based on a polyamide 66 resin. This product is heat stabiised for optimised injection moulding. T..
Tensile Stress 170 MPa

@Strain 2.00 %,
Temperature -40.0 °C
24700 psi

@Strain 2.00 %,
Temperature -40.0 °F
ISO 527
BASF Ultradur B 4300 G6 30% Glass Filled PBT
Ultradur B4300 G6 is an easy flowing injection molding PBT with 30% glass fiber reinforcement for rigid, tough, and dimensionally stable parts.Applications: Program switches, thermostat parts, small..