Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Tensile Stress = 1569 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Stress 10.82 MPa

@Strain 46.76 %,
Temperature 90.0 °C
1569 psi

@Strain 46.76 %,
Temperature 194 °F
TPE; ISO 11403-1 -2
DuPont Performance Polymers Hytrel® 6356 Polyester Elastomer TPC-ET  (Unverified Data**)
63 Shore D High Performance Polyester ElastomerInformation provided by DuPont Performance Polymers
Tensile Stress 10.82 MPa

@Strain 0.260 %,
Temperature 90.0 °C
1569 psi

@Strain 0.260 %,
Temperature 194 °F
50%RH; ISO 11403-1 -2
DuPont Performance Polymers Zytel® 73G30HSL NC010 Nylon 6  (Unverified Data**)
30% Glass Reinforced Heat Stabilized Polyamide 6 Zytel 73G30HSL NC010 is a 30% glass fiber reinforced heat stabilized polyamide 6 resin for injection molding.Information provided by DuPont Performan..