Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 10.82 MPa @Strain 46.76 %, Temperature 90.0 °C |
1569 psi @Strain 46.76 %, Temperature 194 °F |
TPE; ISO 11403-1 -2 |
DuPont Performance Polymers Hytrel® 6356 Polyester Elastomer TPC-ET
(Unverified Data**) 63 Shore D High Performance Polyester ElastomerInformation provided by DuPont Performance Polymers |
|||
Tensile Stress | 10.82 MPa @Strain 0.260 %, Temperature 90.0 °C |
1569 psi @Strain 0.260 %, Temperature 194 °F |
50%RH; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® 73G30HSL NC010 Nylon 6
(Unverified Data**) 30% Glass Reinforced Heat Stabilized Polyamide 6 Zytel 73G30HSL NC010 is a 30% glass fiber reinforced heat stabilized polyamide 6 resin for injection molding.Information provided by DuPont Performan.. |