Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 10.53 MPa @Strain 173.94 %, Temperature 100 °C |
1527 psi @Strain 173.94 %, Temperature 212 °F |
TPE; ISO 11403-1 -2 |
DuPont Performance Polymers Hytrel® 5555HS Polyester Elastomer TPC-ET
(Unverified Data**) 55 Shore D High Performance Polyester Elastomer with Heat Ageing ProtectionInformation provided by DuPont Performance Polymers |
|||
Tensile Stress | 10.53 MPa @Strain 0.900 %, Temperature 80.0 °C |
1527 psi @Strain 0.900 %, Temperature 176 °F |
DAM; ISO 11403-1/-2 |
DuPont Performance Polymers Zytel® FR7026V0F NC010 Nylon 66
(Unverified Data**) Zytel® FR7026V0F NC010 is a flame retardant, heat stabilized, polyamide 66 resin for injection molding. It does not contain elemental phosphorous, halogens or heavy metals.Information provided by D.. |