Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 15.07 MPa @Strain 7.13 %, Temperature 90.0 °C |
2186 psi @Strain 7.13 %, Temperature 194 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Crastin® 6129 NC010 Polybutylene Terephthalate (PBT)
(Unverified Data**) Unreinforced High Viscosity Polybutylene Terephthalate Developed for Extrusion and Injection MoldingInformation provided by DuPont Performance Polymers |
|||
Tensile Stress | 15.07 MPa @Strain 7.13 %, Temperature 90.0 °C |
2186 psi @Strain 7.13 %, Temperature 194 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Crastin® 6130 NC010 Polybutylene Terephthalate (PBT)
(Unverified Data**) Unreinforced High Viscosity Polybutylene Terephthalate Developed for Extrusion and Injection Molding Crastin 6130 NC010 is an unreinforced medium high viscosity polybutylene terephthalate resin for .. |
|||
Tensile Stress | 15.07 MPa @Strain 1.50 %, Temperature 80.0 °C |
2186 psi @Strain 1.50 %, Temperature 176 °F |
DAM; ISO 11403-1/-2 |
DuPont Performance Polymers Zytel® FR7026V0F BK001 Nylon 66
(Unverified Data**) Zytel® FR7026V0F BK001 is a flame retardant heat stabilized polyamide 66 resin for injection molding. It does not contain elemental phosphorous, halogens or heavy metals.Information provided by DuP.. |
|||
Tensile Stress | 15.07 MPa @Strain 8.43 %, Temperature 150 °C |
2186 psi @Strain 8.43 %, Temperature 302 °F |
50%RH; ISO 11403-1 -2 |
DuPont Performance Polymers Minlon® 73M30 NC010 Nylon 6
(Unverified Data**) 30% Mineral Reinforced Polyamide 6 Minlon 73M30 NC010 is a 30% mineral reinforced heat stabilized polyamide 6 resin for injection molding. It has isotropic properties and low warpage.Information pro.. |