Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 11.04 MPa @Strain 2.12 %, Temperature 90.0 °C |
1601 psi @Strain 2.12 %, Temperature 194 °F |
50%RH; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® 7335F NC010 Nylon 6
(Unverified Data**) Unreinforced Polyamide 6 Zytel 7335F NC010 is a nucleated lubricated polyamide 6 resin for injection molding.Information provided by DuPont Performance Polymers |
|||
Tensile Stress | 11.04 MPa @Strain 2.94 %, Temperature 90.0 °C |
1601 psi @Strain 2.94 %, Temperature 194 °F |
DAM; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® RS LC1000 BK385 Nylon 1010 UV Stabilized Renewably Sourced Polyamide 1010 Developed for Extrusion Zytel RS LC1000 BK385 is a renewable sourced Polyamide 1010 containing a minimum of 90% renewably sourced ingredient by weight... |