Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 74.43 MPa @Strain 1.70 %, Temperature 23.0 °C |
10800 psi @Strain 1.70 %, Temperature 73.4 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Delrin® 510GR NC000 Acetal (POM)
(Unverified Data**) 10% Glass Reinforced Medium Viscosity Acetal Homopolymer Delrin 510GR is a 10% glass reinforced acetal homopolymer for injection molding. It has high strength stiffness and high deflection temperatu.. |
|||
Tensile Stress | 74.5 MPa @Strain 0.480 %, Temperature 23.0 °C |
10800 psi @Strain 0.480 %, Temperature 73.4 °F |
ISO 527 |
DuPont Performance Polymers Rynite® FR543 NC010 PET Rynite® FR543 NC010 is a flame retardant, 43% glass reinforced polyethylene terephthalate. Has a 155C temperature index that is equivalent to many thermosets. Recognized by UL as UL94V-0 at 0.8mm.. |
|||
Tensile Stress | 74.49 MPa @Strain 2.80 %, Temperature 90.0 °C |
10800 psi @Strain 2.80 %, Temperature 194 °F |
DAM; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® FR70G25V0 NC010 Nylon 66
(Unverified Data**) 25% Glass Reinforced Flame Retardant Polyamide 66 Zytel FR70G25V0 NC010 is a 25% glass fiber reinforced heat stabilized flame retardant polyamide 66 resin for injection molding.Information provided .. |
|||
Tensile Stress | 74.43 MPa @Strain 0.480 %, Temperature 40.0 °C |
10800 psi @Strain 0.480 %, Temperature 104 °F |
DAM; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® HTN 53G50HSLR NC010 Polyphthalamide (PPA)
(Unverified Data**) 50% Glass Reinforced High Performance Polyamide with Improved Impact and Stiffness Zytel HTN53G50HSLR NC010 is a 50% glass reinforced heat stabilized lubricated high performance polyamide resin deve.. |
|||
Tensile Stress | 74.49 MPa @Strain 0.540 %, Temperature 40.0 °C |
10800 psi @Strain 0.540 %, Temperature 104 °F |
50%RH; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® HTN 53G60LRHF BK083 Polyphthalamide (PPA)
(Unverified Data**) 60% Glass Reinforced High Performance Polyamide with High Stiffness and Improved Flow Zytel HTN53G60LRHF BK083 is a 60% glass reinforced lubricated high performance polyamide resin with improved flo.. |
|||
Tensile Stress | 74.6 MPa @Strain 1.00 %, Temperature 90.0 °C |
10800 psi @Strain 1.00 %, Temperature 194 °F |
DAM; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® HTN FR52G30BL NC010 Polyphthalamide (PPA)
(Unverified Data**) 30% Glass Reinforced Flame Retardant PPA High Performance Polyamide Zytel HTNFR52G30BL NC010 is a 30% glass reinforced flame retardant lubricated high performance polyamide resin that has been devel.. |
|||
Tensile Stress | 74.6 MPa @Strain 1.50 %, Temperature 0.000 °C |
10800 psi @Strain 1.50 %, Temperature 32.0 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Crastin® SK641FR NC010 Polybutylene Terephthalate (PBT) 10% Glass Reinforced Flame Retardant Polybutylene Terephthalate Information provided by DuPont Performance Polymers |
|||
Tensile Stress | 74.8 MPa @Strain 1.20 %, Temperature -40.0 °C |
10800 psi @Strain 1.20 %, Temperature -40.0 °F |
DAM; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® 70G13L NC010 Nylon 66
(Unverified Data**) 13% Glass Reinforced Polyamide 66Zytel 70G13L NC010 is a 13% glass fiber reinforced polyamide 66 resin for injection molding.Information provided by DuPont Performance Polymers |