Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Stress | 1.80 MPa @Strain 100 % |
261 psi @Strain 100 % |
ISO 37 |
PolyOne OnFlex™ S FR 60A-3S1846 Thermoplastic Elastomer (TPE) OnFlex™-S FR thermoplastic elastomer compounds are based on hydrogenated styrenic block copolymers. This range of compounds are specially flame retarded with a highly effective, RoHS compliant halo.. |
|||
Tensile Stress | 1.80 MPa @Strain 300 %, Temperature 23.0 °C |
261 psi @Strain 300 %, Temperature 73.4 °F |
Die C2 hr; ASTM D412 |
PolyOne Versaflex™ OM 9-801N Thermoplastic Elastomer (TPE) Versaflex™ OM 9-801N is designed for overmolding onto a wide variety of substrates including PC, ABS, PC/ABS, HIPS, PPO, acetal, acrylic and copolyester. - Bonds to a Variety Of Substrates - Rubber.. |
|||
Tensile Stress | 1.80 MPa @Strain 100 % |
261 psi @Strain 100 % |
ASTM D412 |
Polymax® Maxelast® P3953CT TPE, PP Overmold or Standalone use Polymax's TPE material complies with UL, VDE, FDA, RoHS and PAH's standards.Uses:Consumer ProductsToys & NoveltiesAuto PartsTool Hand GripsSporting GoodsWire & Cable ElectronicsMedical DevicesPlasti.. |
|||
Tensile Stress | 1.80 MPa @Strain 10.0 % |
261 psi @Strain 10.0 % |
ISO 527-1/-2 |
DuPont Performance Polymers Hytrel® 3078 Polyester Elastomer TPC-ET
(Unverified Data**) 30 Shore D High Performance Polyester Elastomer with Non-discoloring Stabilizer Hytrel 3078 is a very low modulus grade with nominal hardness of 30D. It contains non-discoloring stabilizer. It can b.. |
|||
Tensile Stress | 1.80 MPa @Strain 10.0 %, Temperature 23.0 °C |
261 psi @Strain 10.0 %, Temperature 73.4 °F |
ISO 11403-1 -2 |
DuPont Performance Polymers Hytrel® 3078 Polyester Elastomer TPC-ET
(Unverified Data**) 30 Shore D High Performance Polyester Elastomer with Non-discoloring Stabilizer Hytrel 3078 is a very low modulus grade with nominal hardness of 30D. It contains non-discoloring stabilizer. It can b.. |
|||
Tensile Stress | 1.80 MPa @Strain 0.281 %, Time 360000 sec |
261 psi @Strain 0.281 %, Time 100 hour |
50%RH; isochronous; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® 7335F NC010 Nylon 6
(Unverified Data**) Unreinforced Polyamide 6 Zytel 7335F NC010 is a nucleated lubricated polyamide 6 resin for injection molding.Information provided by DuPont Performance Polymers |
|||
Tensile Stress | 1.80 MPa @Strain 0.308 %, Time 3.60e+6 sec |
261 psi @Strain 0.308 %, Time 1000 hour |
50%RH; isochronous; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® 7335F NC010 Nylon 6
(Unverified Data**) Unreinforced Polyamide 6 Zytel 7335F NC010 is a nucleated lubricated polyamide 6 resin for injection molding.Information provided by DuPont Performance Polymers |
|||
Tensile Stress | 1.80 MPa @Strain 0.182 %, Time 3600 sec |
261 psi @Strain 0.182 %, Time 1.00 hour |
50%RH; isochronous; ISO 11403-1 -2 |
DuPont Performance Polymers Zytel® 7335F NC010 Nylon 6
(Unverified Data**) Unreinforced Polyamide 6 Zytel 7335F NC010 is a nucleated lubricated polyamide 6 resin for injection molding.Information provided by DuPont Performance Polymers |
|||
Tensile Stress | 1.80 MPa @Strain 10.0 %, Temperature 100 °C |
261 psi @Strain 10.0 %, Temperature 212 °F |
ISO 527 (1BA bar) |
DuPont Performance Polymers Hytrel® HTR8636 NC010 TPC-ET
(Unverified Data**) Hytrel® HTR8636 NC010 is a medium modulus Hytrel® grade with nominal durometer hardness of 40D. It contains non_discoloring stabilizer. It is specially suitable for extrusion processing.Informatio.. |
|||
Tensile Stress | 1.80 MPa @Strain 100 % |
261 psi @Strain 100 % |
ISO 37 |
Alliance Polymers Viprene™ P50A-22U-BLK Thermoplastic Vulcanizate Elastomer Viprene™ P50A-22U-BLK is a UV and Heat Stabilized TVP (Thermoplastic Vulcanizate Elastomer). This material can be easily processed by extrusion or injection molding. It exhibits easy flowing charac.. |
|||
Tensile Stress | 1.80 MPa @Strain 100 % |
261 psi @Strain 100 % |
ISO 37 |
Alliance Polymers Viprene™ P50A-22U-NAT Thermoplastic Vulcanizate Elastomer Viprene™ P50A-22U-NAT is a UV and Heat Stabilized TVP (Thermoplastic Vulcanizate Elastomer). This material can be easily processed by extrusion or injection molding. It exhibits easy flowing charac.. |